Products/JIS G4804

MATERIAL DATA · COLD FORMING

SUM42 cold heading wire rod

Technical data for SUM42 cold heading wire rod, compliant with JIS G4804. View the chemical composition, mechanical properties, and related technical requirements for this grade.

SUM42 cold heading wire rod product image
SUM42 · Cold forming wire rod
01StandardJIS G4804
02GradeSUM42
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 -- Chemical Composition, %

GradeCMnPSPb
SUM420.37~0.451.35~1.65<0.0400.08~0.13
Note a) Si is not specified. However, upon agreement between supplier and purchaser, limits or ranges such as ≤0.10%, 0.10%–0.20%, or 0.15%–0.35% may be established.
b) Elements not specified in this table shall not be intentionally added to the steel, except for the purpose of completing the steelmaking process, unless agreed upon by the supplier and purchaser.
c) For SUM22 and SUM22L, the upper limit for Mn may be set at 1.10% upon agreement between the supplier and the purchaser.
d) When product analysis for lead in leaded steel is conducted at the purchaser's request, the lead content shall be 0.07–0.35%.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.