Products/JIS G4805

MATERIAL DATA · COLD FORMING

SUJ4 wire rod for cold forming

Technical data for SUJ4 wire rod for cold forming, compliant with JIS G4805. View the chemical composition, mechanical properties, and related technical requirements for this grade.

SUJ4 wire rod for cold forming product image
SUJ4 · Cold forming wire rod
01StandardJIS G4805
02GradeSUJ4
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 -- Chemical Composition, %

GradeCSiMnPSCrMoNiCu a)
SUJ40.95~1.100.15~0.35≤0.50≤0.025≤0.0251.30~1.600.10~0.25≤0.25≤0.25
Elements not specified in this table shall not be intentionally added except for the purpose of finishing the molten steel, unless agreed upon between the parties involved. Note a) The Cu content in wire rod shall be 0.20% or less.
Elements not specified in this table shall not be intentionally added except for steelmaking purposes; any such addition shall be determined by agreement between the supplier and the purchaser.
Note a) The Cu content in wire rod shall be 0.20% or less.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

3. Dimensional Tolerances

4. Permissible Limits for Total Decarburized Layer Depth

Table 9 - Permissible Limits for Total Decarburized Layer Depth (Cold-Drawn Steel)

Cold-Drawn Round BarCold-Drawn Wire
DiameterTotal decarburized layer depth from the surfaceDiameterTotal decarburized layer depth from the surface
<15<0.20≤7<0.05
15<d≤25<0.257<d≤15<0.08
25<d≤35<0.3015<d≤20<0.10
Permissible tolerances for cold-drawn round steel with diameters exceeding 35 mm and cold-drawn steel wire with diameters exceeding 20 mm shall be subject to agreement between the supplier and the purchaser.

5. Hardness

Table 10 – Spheroidizing annealing hardness (rolled steel for machining)

GradeHardness
HBWHRBHV
SUJ2,SUJ4<201<94<218
For hot-rolled steel for machining that has undergone spheroidizing annealing, testing is performed in accordance with Clause 14.3, and hardness is expressed as Brinell hardness (HBW), Rockwell hardness (HRBW), or Vickers hardness (HV) as specified in Table 10. However, Vickers hardness (HV) applies only to diameters of 17 mm or less. The hardness of cold-drawn steel and the low-temperature annealing hardness of steel for forging shall be subject to agreement between the supplier and the purchaser.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.