Products/ISO 4954

MATERIAL DATA · COLD FORMING

Custom shaped wire for automotive seatbelt locking blocks

Technical data for custom shaped wire for automotive seatbelt locking blocks, compliant with ISO 4954-Annex A. View the chemical composition, mechanical properties, and related technical requirements for this grade.

Custom shaped wire for automotive seatbelt locking blocks product image
Custom shaped wire for automotive seatbelt locking blocks · Custom shaped wire
01StandardISO 4954
02GradeCustom shaped wire for automotive seatbelt locking blocks
03Product formCustom shaped wire
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Available material list

Available material list

ApplicationsMaterial No.DIN EN ISOASTM/AISIJIS
1.0304AISI 1008SWRM 8
1.031AISI 1010SWRM 10
1.0541AISI 1040SWRH 42A
1.0517AISI 1045SWRH 47A
1.0609SWRH 57A
1.0611SWRH 62A
1.0620SWRH 77B
1.0626SWRH 82A
1.0737AISI 12L14SUM24L
1.0762AISI 1144SUM43
1.7243SAE 4118SCM415
1.7220SAE 4135SCM435
1.722542CrMo4SAE 4140SCM440
1.652320CrNiMo2-2SAE 8620SNCM220
1.815951CrV4SAE 6150SUP10
1.7104SAE 9254SUP12
1.2067100Cr6SAE 52100SUJ2
Structural steel1.0038S235JR1015SS330
1.0577S355J2A738
1.0050E295S490
1.0060E335SM570
Free-cutting steel1.071511SMn301213、1215SUM22
1.071811SMnPb3012L13SUM22L
1.072635S201140
1.072746S201146
Heat-treatable steel1.0503C451043、1045S45CM,S45C
1.0601C601060S60CM,S60C
1.721825CrMo44130SCM430
1.722542CrMo44140SCM440
Roller bearing steel and tool steel1.779258CrMoV4
1.3505100Cr6E52100SUJ2
1.1213C53G1050、1055S50CM,S50C
1.284290MnCrV8A681
1.717760Cr3
1.815951CrV46145SUP10
Case-hardening steel and nitriding steel1.0401C151015、1017S15C
1.713116MnCr55115
1.591817CrNi6-6
1.592018CrNi8
1.652320CrNiMo2-28617\8620SNCM220
1.2764X19NiCrMo4
1.575215NiCr133310SNC815
1.851931CrMoV9

2. Surface quality

2.1 Hot-rolled profiles

Surface quality in accordance with standard EN 10163-3 or other national standards (ASTM, GB, JIS)
Surface roughness: Ra < 40 microns
Dimensional tolerance: max. 0.5 mm
Straightness: Standard s
1.0 mm/m; < 0.3 mm/m upon request
Twist: Standard 1/m; upon request ≤ 0.5/m
Cross-section: 10mm - 7000mm
Length: ≤ 12 m or cut to fixed lengths

2.2 Cold-rolled/cold-drawn profiles

Surface quality in accordance with EN 10277-1 or other national standards (ASTM, GB, JIS)
Surface roughness: Ra ≤
2.5 microns
Decarburization: ≤ 0.1mm
Straightness: ≤ 0.1mm/m
Twist: 0.25°/m
Dimensional tolerance: ≤ 0.05mm
Cross-section: 1mm - 3800mm
Length: ≤ 6 m or cut to fixed length

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

What to include in the enquiry

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →