Products/JIS G4107

MATERIAL DATA · COLD FORMING

SNB5 Wire Rod for Cold Forming

Technical data for SNB5 wire rod for cold forming, compliant with JIS G4107. View chemical composition, mechanical properties, and related technical requirements for the current grade.

SNB5 Wire Rod for Cold Forming product image
SNB5 · Cold forming wire rod
01StandardJIS G4107
02GradeSNB5
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 3 -- Chemical Composition (Ladle Analysis)

Note a) Elements not specified in this table shall not be intentionally added to the steel, except for the purpose of completing the melt, unless agreed upon by both the supplier and the purchaser.
b) For SNB7, the upper limit of carbon content may be 0.50% when the diameter of the bolt material exceeds 90 mm.

2. Mechanical properties of wire rod

Table 4 -- Mechanical Properties

3. Dimensional Tolerances

Table 6 -- Dimensional Tolerances for Hot-Rolled Wire Rod

DiameterDiameter toleranceOut-of-roundness
<15±0.3<0.4
15<d≤25±0.4<0.5
25<d≤32±0.5<0.6
32<d≤50±0.6<0.7
For diameters exceeding 50 mm, subject to agreement between supplier and purchaser.
Note a) Out-of-roundness refers to the difference between the maximum and minimum diameters measured on the same cross-section of the wire rod.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.