Products/JIS G4053

MATERIAL DATA · COLD FORMING

SMn438 Steel for cold forming

Technical data for SMn438 Steel for cold forming, compliant with JIS G4053. View the chemical composition, mechanical properties, and related technical requirements for this grade.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

SMn438 Steel for cold forming
SMn438 · Steel for cold forming
01Applicable standardJIS G4053
02Material gradeSMn438
03Product formSteel for cold forming
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

Composition source and applicability

Reference composition for the stated standard edition, not heat analysis. Confirm the order standard and the separate requirements for feedstock and finished product.

SMn438 · JIS G 4053-2008

SMn438 · JIS G 4053-2008 · Mass fraction / %
ElementMass fraction / %
C0.35–0.41
Si0.15–0.35
Mn1.35–1.65
P≤0.03
S≤0.03
Ni≤0.25
Cr≤0.35
Cu≤0.3
Source: JIS G 4053-2008
Composition source and applicability · JIS G 4053-2008 · PDF 5
JIS G 4053-2008 · PDF 5
Composition source and applicability · JIS G 4053-2008 · PDF 6
JIS G 4053-2008 · PDF 6

1. Chemical Composition

Table 2 - Chemical composition, unit %

Elements not specified in this table shall not be intentionally added, except where necessary for steelmaking purposes.
Note a) Shall not be intentionally added.
b) For SNCM630, the lower limit for Mo may be 0.30% upon agreement between supplier and purchaser.
c) Al content for SACM645 is 0.70% ~ 1.20%.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

3. Dimensional Tolerances

Table 8 - Dimensional tolerances for hot-rolled wire rod

DiameterDiameter toleranceOut-of-roundness
<15±0.3<0.4
15<d≤25±0.4<0.5
25<d≤32±0.5<0.6
32<d≤50±0.6<0.7
Tolerances for wire rod with a diameter exceeding 50 mm shall be determined by agreement between the supplier and the purchaser.
Note a) Out-of-roundness refers to the difference between the maximum and minimum diameters measured on the same cross-section of the wire rod.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — SMn438

Basis: JIS G4053

Chemical composition source: JIS G 4053-2008

Transcribed from the cited standard

The product does not specify a standard edition. Composition uses the verified source edition explicitly cited here. Confirm the contract edition separately; do not assume other editions are identical.

Original source wording

Table 2 and its continuation, Notes a/b; Clause 5

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 0.5750–0.7917

Missing elements: Mo, V

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 0.4225–0.5408

Missing elements: Mo, V, B

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Known-element contribution, not a complete value: 0.4850–0.6137

Missing elements: Mo

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →
Image and content use · Creation Group