Pierce Nut Profile Wire
Material identification10B21
Section CategoryPierce Nut Profile Wire – non-circular cross-section
Recorded nominal dimensions / mmConfirm according to the drawing

Geometric Focus Points

Shoulder, sidewall, and bottom profile

Cross-section dimensions, sidewall angles, and radii to be confirmed per drawing.

Confirm technical requirements based on the drawing

Cross-sectional features and review points

10B21 Pierce Nut Profile Wire sample highlights shoulder, sidewall, and bottom profile, illustrated in context of automotive side-door window regulator installation.

Drawings and measurement requirements

Review shall separately verify cross-sectional width/height, shoulder height, bottom width, sidewall angle, and local steps; MAX fillets and fine steps in the model represent approximate reconstruction.

Automotive Side-Door Window Regulator Installation

Application-scenario photographs show the side-door window regulator assembly and its installation environment inside the vehicle door. Final hole dimensions, thread specifications, and assembly requirements shall be verified per the component drawing.

Documentation basis and scope of confirmation

Data originates from this case’s catalog and internal sample photographs; catalog dimensions are nominal values, and photographs do not substitute formal inspection reports. Material standards, mechanical properties, heat treatment, supply conditions, and acceptance criteria must be confirmed per project.

Interactive 3D model

3D reference model; actual dimensions and manufacturing conditions to be confirmed per drawing.

Photo recording

10B21 Pierce Nut Profile Wire · Sample Photograph 1
10B21 Pierce Nut Profile Wire · Sample Photograph 1 · 1 / 4
10B21 Pierce Nut Profile Wire · Sample Photograph 2
10B21 Pierce Nut Profile Wire · Sample Photograph 2 · 2 / 4
Close-Up View of the Automotive Side-Door Window Regulator Assembly
Close-Up View of the Automotive Side-Door Window Regulator Assembly · 3 / 4
Installation Environment of the Window Regulator Inside the Automotive Side Door
Installation Environment of the Window Regulator Inside the Automotive Side Door · 4 / 4

Development Q&A

Does the pierce nut case model already include finished thread requirements?

No. This page displays a reference cross-sectional model for wire; finished holes, threads, and their manufacturing and inspection requirements must be defined separately in subsequent part drawings.

How should shoulder and sidewall be verified?

Verify shoulder height, sidewall angle, bottom width, and step dimensions separately against the approved drawing; confirm local fillets and measurement datum. Approximate models must not substitute for acceptance verification.

Related cross-sectional cases

Material data and technical communication

Technical requirements must include cross-sectional drawing and revision, critical tolerances, subsequent processing steps, delivery form, and inspection requirements.

View material selection documentation Submit technical requirements ↗

← Return to all cases

WhatsApp Technical enquiry →
Image and content use · Creation Group