Products/JIS G4053

MATERIAL DATA · COLD FORMING

SCr430 Wire Rod for Cold Forming

Technical data for SCr430 wire rod for cold forming, compliant with JIS G4053. View the chemical composition, mechanical properties, and related technical requirements for the current grade.

SCr430 Wire Rod for Cold Forming product image
SCr430 · Cold forming wire rod
01StandardJIS G4053
02GradeSCr430
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 2 - Chemical composition, unit %

GradeCSiMnPSNiCrMoCu
SCr4300.28 ~ 0.330.15 ~ 0.350.60 ~ 0.90≤0.030≤0.030≤0.250.90 ~ 1.20–<0.30
Elements not specified in this table shall not be intentionally added, except where necessary for steelmaking purposes.
Note a) Shall not be intentionally added.
b) For SNCM630, the lower limit for Mo may be 0.30% upon agreement between supplier and purchaser.
c) Al content for SACM645 is 0.70% ~ 1.20%.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

3. Dimensional Tolerances

Table 8 - Dimensional tolerances for hot-rolled wire rod

DiameterDiameter toleranceOut-of-roundness
<15±0.3<0.4
15<d≤25±0.4<0.5
25<d≤32±0.5<0.6
32<d≤50±0.6<0.7
Tolerances for wire rod with a diameter exceeding 50 mm shall be determined by agreement between the supplier and the purchaser.
Note a) Out-of-roundness refers to the difference between the maximum and minimum diameters measured on the same cross-section of the wire rod.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

What to include in the enquiry

Send a technical enquiry

Contact technical team →