Products/JIS G3509

MATERIAL DATA · COLD FORMING

SCM425WCH Wire Rod for Cold Forming

Technical data for SCM425WCH cold heading wire rod, compliant with JIS G3509. View the chemical composition, mechanical properties, and related technical requirements for this grade.

SCM425WCH Wire Rod for Cold Forming product image
SCM425WCH · Cold forming wire rod
01StandardJIS G3509
02GradeSCM425WCH
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 – Chemical composition, unit: %

For all steel grades listed in this table, the Cu content as an impurity shall not exceed 0.30%.
Al may be added for grain refinement upon agreement between the supplier and the purchaser.
Elements not specified in this table shall not be intentionally added except for steelmaking purposes; any such addition shall be determined by agreement between the supplier and the purchaser.
Upon agreement between the supplier and the purchaser, the permissible deviations from the specified values for ladle analysis during product analysis of steel shall comply with Table 4 of JIS G 0321.
Note a) The lower limit for Si may be set to a value below 0.15% upon agreement between the supplier and the purchaser.

2. Mechanical properties of wire rod

Table 2 – Mechanical properties of wire rod

GradeTensile strength (N/mm²)Reduction of area (%)
DA1DA2DA3DA1DA2DA3
SCM425WCH≤650≤600≤550≥55≥60≥60

3. Depth of decarburized layer

Table 3 Permissible limits for average decarburized layer depth

Unit: mm
DiameterFerrite decarburized layer depthTotal decarburized layer depth
≤15≤0.02≤0.12
>15~25≤0.02≤0.15
>25~32≤0.02≤0.20
>32~40≤0.03≤0.25
>40~50≤0.03≤0.30
For wire rod with a diameter exceeding 50 mm, to be agreed upon by both supplier and purchaser.

4. Hardenability

Table 5 Distance from quenched end and hardness

5. Wire diameter tolerance and out-of-roundness

Table 8 Wire diameter tolerance and out-of-roundness

DiameterPermissible deviationOut-of-roundness
≤15±0.30≤0.40
>15~25±0.40≤0.50
>25~32±0.50≤0.60
>32~50±0.60≤0.70
Note 1) Diameter deviation refers to the difference between the maximum and minimum diameters within the same cross-section of the wire rod. For wire rods with a diameter exceeding 50 mm, this shall be subject to agreement between the supplier and the purchaser.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

What to include in the enquiry

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →