S35C · Cold forming wire rod
01StandardJIS G4051
02GradeS35C
03Product formCold forming wire rod
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 2 - Chemical composition, unit %

GradeCSiMnPSNiCr a)CuNi+Cr b)
S35C0.32~0.380.15~0.350.60~0.90≤0.030≤0.035≤0.20≤0.20≤0.30≤0.35
Elements not specified in this table shall not be intentionally added, except where necessary for steelmaking purposes.
Note a) May be less than 0.30% upon agreement between supplier and purchaser.
b) Upon agreement between supplier and purchaser, the upper limit for Ni + Cr is less than 0.40% for S09CK, S15CK, and S20CK; for other grades, it may also be less than 0.45%.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

3. Dimensional Tolerances

Table 8 - Dimensional tolerances for hot-rolled wire rod

DiameterDiameter toleranceOut-of-roundness a)
<15±0.3<0.4
15<d≤25±0.4<0.5
25<d≤32±0.5<0.6
32<d≤50±0.6<0.7
Tolerances for wire rod with a diameter exceeding 50 mm shall be determined by agreement between the supplier and the purchaser.
Note a) Out-of-roundness refers to the difference between the maximum and minimum diameters measured on the same cross-section of the wire rod.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

What to include in the enquiry

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →