Products/JIS G4051

MATERIAL DATA · COLD FORMING

S20C Steel for cold forming

Technical data for S20C wire rod for cold forming, compliant with JIS G4051. View the chemical composition, mechanical properties, and related technical requirements for this grade.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

S20C Steel for cold forming
S20C · Steel for cold forming
01Applicable standardJIS G4051
02Material gradeS20C
03Product formSteel for cold forming
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 2 - Chemical composition, unit %

GradeCSiMnPSNiCr a)CuNi+Cr b)
S20C0.18~0.230.15~0.350.30~0.60≤0.030≤0.035≤0.20≤0.20≤0.30≤0.35
Elements not specified in this table shall not be intentionally added, except where necessary for steelmaking purposes.
Note a) May be less than 0.30% upon agreement between supplier and purchaser.
b) Upon agreement between supplier and purchaser, the upper limit for Ni + Cr is less than 0.40% for S09CK, S15CK, and S20CK; for other grades, it may also be less than 0.45%.

2. Mechanical properties of wire rod

Mechanical property values shall be determined by agreement between the supplier and the purchaser.

3. Dimensional Tolerances

Table 8 - Dimensional tolerances for hot-rolled wire rod

DiameterDiameter toleranceOut-of-roundness a)
<15±0.3<0.4
15<d≤25±0.4<0.5
25<d≤32±0.5<0.6
32<d≤50±0.6<0.7
Tolerances for wire rod with a diameter exceeding 50 mm shall be determined by agreement between the supplier and the purchaser.
Note a) Out-of-roundness refers to the difference between the maximum and minimum diameters measured on the same cross-section of the wire rod.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — S20C

Basis: JIS G4051

Chemical composition source: JIS G 4051-2023

Transcribed from the cited standard

The product does not specify a standard edition. Composition uses the verified source edition explicitly cited here. Confirm the contract edition separately; do not assume other editions are identical.

Original source wording

Table 2 and Notes a/b; Clause 6

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15

Confirm the applicable product conditions before calculating the carbon equivalent.

  • Product dimensions or processing conditions

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B

Confirm the applicable product conditions before calculating the carbon equivalent.

  • Product dimensions or processing conditions

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40

Confirm the applicable product conditions before calculating the carbon equivalent.

  • Product dimensions or processing conditions

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →
Image and content use · Creation Group