Products/GB/T 5953

MATERIAL DATA · COLD FORMING

ML06Al Cold heading wire

Technical data for ML06Al Cold heading wire, compliant with GB/T 5953. View the chemical composition, mechanical properties, and related technical requirements for this grade.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

ML06Al Cold heading wire
ML06Al · Cold heading wire
01Applicable standardGB/T 5953
02Material gradeML06Al
03Product formCold heading wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical Composition

Table 1 – Chemical composition, mass fraction %

No.Unified digital codeGradeChemical composition (mass fraction)/%
CSiMnPSAlₜ
2U40068ML06Al≤0.08≤0.100.30〜0.60≤0.035≤0.035≥0.020
When determining acid-soluble aluminum Al, Al≥0.015%.
When determining acid-soluble aluminum Al, Al≥0.015%.

2. Mechanical Properties

Table 2 Tensile strength, reduction of area, and hardness of HD process steel wire


2.1 For cold heading wire produced by the HD process, tensile strength and reduction of area shall comply with the requirements specified in Table 2.

Note: For wire with a nominal diameter greater than 20 mm, the reduction of area may be reduced by 5%. a) The chemical composition of the grades may refer to GB/T 6478. b) Hardness values are for reference only.

Table 3 Tensile strength, reduction of area, and hardness of wire produced by the SALD process


2.2 For cold heading wire produced by the SALD process, the tensile strength and reduction of area shall comply with the requirements specified in Table 3.

Note: For wire with a nominal diameter greater than 20 mm, the reduction of area may be reduced by 5%. a) The chemical composition of the grades may refer to GB/T 6478. b) Hardness values are for reference only.
2.3 The mechanical properties of wire with a nominal diameter greater than 25.00 mm shall be determined by agreement between the supplier and the purchaser.
2.4 The mechanical properties of wire grades not listed in the table shall be determined by agreement between the supplier and the purchaser.
2.5 Upsetting Cold heading wire produced by the HD process: Wire samples shall show no cracks or fissures after being cold upset to one-half of their original height. Cold heading wire produced by the SALD process: Wire samples shall show no cracks or fissures after being cold upset to one-third of their original height. No upsetting test is required for wire with a diameter ≤ 5.0 mm.

3. Microstructure

Table 4 Permissible range for decarburized layer depth

Table 4 Permissible range for decarburized layer depthUnit: mm
Nominal wire diameter/dDepth of complete decarburizationTotal decarburized layer depth
<10.00≤0.02≤0.01 d
≥10.00—15.00≤0.02≤0.15
≥15.00〜25.00≤0.03≤0.20
Note: When the nominal wire diameter exceeds 25.00 mm, the permissible range for decarburized layer depth shall be determined by agreement between the supplier and the purchaser.

6.1 Microstructure For wire produced by the SALD process, the microstructure shall be spheroidized. The spheroidizing grade shall be agreed upon by the supplier and the purchaser and assessed in accordance with JB/T 5074. The test method for the decarburized layer shall be determined by agreement between the supplier and the purchaser.
6.2 Decarburized layer depth Wire produced by the SALD process shall undergo decarburization testing. The permissible ranges for the depth of complete decarburization on one side and the total decarburized layer depth (ferrite + transition layer) shall comply with the provisions of Table 4. The test method for the decarburized layer shall be determined by agreement between the supplier and the purchaser.
6.3 Carburization Wire produced by the SALD process shall not exhibit surface carburization. Testing may be omitted if guaranteed by the supplier.

4. Comparison table of non-heat-treated cold heading steel grades with domestic and international equivalents; see Table B.1 for grade comparisons.

Table B.1 Cross-reference of non-heat-treated cold heading steel grades with domestic and international equivalents

Unified digital codeThis standardGB/T 6478ISO 4954EN 10263-2JIS G3507-1ASTM A29/A29M
U40068ML06Al---SWRCH6A1006

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — ML06Al

Basis: GB/T 5953

Chemical composition source: GB/T 6478-2015

Transcribed from the cited standard

Original source wording

Table 1

IIW / CEV

CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15Known-element contribution, not a complete value: 0.0500–0.2467

Missing elements: Mo, V

IIW/CEV: carbon and low-alloy steel weldability screening.

Pcm (Ito–Bessyo)

Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5BKnown-element contribution, not a complete value: 0.0150–0.1367

Missing elements: Mo, V, B

Pcm: mainly low-carbon, low-alloy steels; confirm applicability, particularly when C exceeds 0.11%.

CET

CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40Known-element contribution, not a complete value: 0.0300–0.1650

Missing elements: Mo

CET: ferritic-steel preheat assessment; confirm EN 1011-2 conditions.

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →

Send a technical enquiry

Contact technical team →

Material reference data

Same-grade reference does not establish standard equivalence, supply or substitution approval.

WhatsApp Technical enquiry →