Products/ASTM F2282-23 / IFI

MATERIAL DATA · COLD FORMING

IFI-1541/B CHQ wire

Data reference: ASTM F2282-23. Delivery condition and acceptance requirements are confirmed in the order specification.

Cold-formed component illustration; not a verified specimen of this grade.
Cold-formed component illustration; not a verified specimen of this grade.
01Applicable standardASTM F2282-23 / IFI
02Material gradeIFI-1541/B
03Product formCold heading wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical composition

ElementMass fraction %
C0.38–0.43
Mn1.35–1.60
P≤ 0.020
S≤ 0.020
Si0.15–0.30 (SiFg/SiCg); CgP: confirm practice

2. Mechanical properties

Delivery conditionRm ≤ / ksiR/A ≥ / %
Rod/bar: annealed9353
Rod/bar: spheroidize annealed8657
Wire: SAFS8361
Wire: AIP9951
Wire: SAIP9355

3. Source clauses and scope

Data reference: ASTM F2282-23. Delivery condition and acceptance requirements are confirmed in the order specification.

ASTM F2282-23 Table 4 names the permitted steelmaking practices; Table 6 gives Si 0.15–0.30% for the Si-killed fine/coarse-grain practices of these grades. IFI-1541/B also lists CgP; the order must identify the actual deoxidation practice before a Si limit is applied to that option.

ASTM F2282-23 Table 4 steelmaking practices for this grade: SiFg / SiCg / CgP. SiFg = silicon-killed fine grain; SiCg = silicon-killed coarse grain; CgP = coarse-grain practice. These are not equivalence claims.

ASTM F2282-23 Table 11: maximum tensile strength in ksi and minimum reduction of area (R/A) in percent. Material condition and product form determine the applicable column.

Table 11 footnote A: for aluminium-killed steel subtract 3 ksi and add 1 percentage point R/A; for rimmed steel subtract 5 ksi and add 2 percentage points R/A.

For AIP and SAIP wire below 0.200 in., Table 11 footnote A adds 50 psi for every 0.001 in. below 0.200 in.; apply only to those two columns.

Table 11 Note 1: R/A testing does not apply to wire below 0.092 in. These tabulated limits are not a mill certificate or order-specific acceptance decision.

ASTM F2282-23 section 6.5 also requires the residual-element limits in Table 9. Table 4 does not repeat those limits in each grade row; this page is not a substitute for the complete ordered specification.

ASTM reference: F2282-23 · Tables 4, 6, 10 and 11. Historical page identity: IFI-1541/B.

ASTM F2282-23 Table 10 · Decarburization · inches

Diameter d / in.Free ferrite depth ≤ / in.TAAD ≤ / in.Worst-location depth ≤ / in.
d ≤ 25/640.0010.0050.008
25/64 < d ≤ 5/80.0010.0060.009
5/8 < d ≤ 55/640.0010.0070.011
55/64 < d ≤ 10.0010.0080.012
1 < d ≤ 1½0.0010.0100.015

Table 10 applies to killed steels with carbon content exceeding 0.15%. Confirm the ordered product form and applicable acceptance method; the page is not a mill certificate.

Application and ordering note

Data reference: ASTM F2282-23. Delivery condition and acceptance requirements are confirmed in the order specification.