Products/GB/T 5953-2026

MATERIAL DATA · COLD FORMING

ML20MnA Cold-Heading Steel Wire

ML20MnA cold-heading steel wire: ML20Mn chemistry is shown as the confirmed reference; requirements for the A designation, finished-wire properties and delivery are subject to the order technical agreement and applicable GB/T 5953 edition.

Supply and technical review · Creation Group accepts supply and technical review enquiries for this product. Dimensions, delivery condition, quantity and inspection documents are confirmed in the order technical agreement after review.

ML20MnA illustrative product form
ML20MnA · Illustrative product form; not evidence of this grade or any batch.
01Applicable standardGB/T 5953
02Material gradeML20MnA
03Product formCold heading wire
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

1. Chemical composition (cast analysis)

Source: GB/T 28906-2025, Table 2, ML20Mn (reference basis confirmed by the user); PDF page 8. Mass fractions are expressed in %.

ElementMass fraction / %
C0.18-0.23
Si≤0.10
Mn0.70-1.00
P≤0.025
S≤0.020
Al_t0.020-0.060

ML20MnA is not listed separately in GB/T 28906-2025. This page uses ML20Mn as a reference, as confirmed by the user. Any tighter P, S and cleanliness requirements associated with A shall be specified in the order technical agreement. The P and S values shown are reference limits and do not establish confirmed tighter limits.

GB/T 28906-2025, Table 2, note b: where acid-soluble aluminium Al_s is determined, its specified range is 0.015%–0.055%. This is distinct from the total aluminium Al_t range shown above.

GB/T 28906-2025, 7.1.5: residual Ni, Cr and Cu shall each be ≤0.20%, and residual Mo ≤0.06%; the explicitly specified alloy-element limits for the grade take precedence. Permissible deviations in product analysis are governed by GB/T 222. The composition basis and finished-wire requirements are listed separately.

2. Finished-wire properties · GB/T 5953-2026

Published on 2026-05-25; effective from 2026-12-01. This page presents that edition. The edition and delivery condition applicable to an order must be specified.

Delivery conditionNominal diameter d / mmRm / MPaZ / %Hardness (reference only for SA, SALD and ASALD)Rp0.2 / MPaA / %Source
SA≤520≥60≤82 HRBWTable 3; PDF page 8
SALDd≤6.00440-640≥55Table 4; PDF page 11
SALD6.00<d≤12.00420-600≥55Table 4; PDF page 11
SALD12.00<d≤25.00400-550≥50≤85 HRBWTable 4; PDF page 11

A blank cell means that the row does not specify a value; it does not mean zero. Do not apply properties from another grade or an HD, SA, SALD or ASALD condition not listed for this grade. For diameters greater than 20 mm, reduction of area Z is reduced by 5% in accordance with the applicable table note. Hardness is for reference only in SA, SALD and ASALD conditions; the HD hardness requirements in Table 2 apply. For delivery in straight lengths or in a polished condition, a 10% variation in mechanical properties is permitted. Mechanical properties may also be agreed between purchaser and supplier (6.5.5–6.5.6).

SA: cold drawing + spheroidizing annealing. SALD: cold drawing + spheroidizing annealing + light drawing. ASALD: annealing + cold drawing + spheroidizing annealing + light drawing. The delivery condition shall be specified in the contract. Table 5 note: reduction of area for d<3.00 mm is for reference only (this page contains no Table 5 property row).

3. Dimensions, shape and coil mass

6.4: nominal diameter 1.00–45.00 mm. For d≤20.00 mm, diameter tolerance is grade 10 in GB/T 342-2017, Table 2; for 20.00<d≤25.00 mm, grade 11 in GB/T 702-2026, Table 9; for d>25.00 mm, by agreement. Out-of-roundness shall not exceed 1/2 of the diameter tolerance.

Polished wire in straight lengths: grade 10 of GB/T 3207-2025 for d≤16.00 mm and grade 11 for 16.00<d≤25.00 mm; for d>25.00 mm, by agreement. Coils shall be orderly and free of distortion that impairs use. Straight lengths are normally 2000–6000 mm, with straightness deviation ≤2 mm/m.

Nominal diameter d / mmMinimum coil mass / kg
1.00≤d≤2.0020
2.00<d≤5.0030
5.00<d≤6.5050
d>6.50100

Each coil shall consist of one continuous length of wire without joints of any kind. Where a nominal coil mass of 100–2500 kg is agreed, the permitted mass deviation is ±15%. The mass of wire in straight lengths is by agreement.

4. Surface quality, upsetting test and microstructure

6.3: the wire surface shall be smooth and free of cracks, folds, scabs, laminations, drawing marks, hairline cracks and rust that impair cold heading or cold forming. Isolated pits and depressions shall be no deeper than 1/2 of the diameter tolerance; isolated indentations and scratches that do not impair use shall be no deeper than 1/4 of the diameter tolerance. Surface coatings are by agreement.

6.6: HD wire shall withstand upsetting to 1/2 of the original specimen height; SA, SALD and ASALD wire to 1/3, without cracks or splits. The upsetting test is not required for d≤5.0 mm. Under 6.7, SA, SALD and ASALD wire shall have a spheroidized microstructure rated at least grade 4 in accordance with GB/T 38770.

5. Decarburization depth

6.8: decarburization is inspected for SA, SALD and ASALD wire with average C≥0.30%. Values below are depths measured from one side of the wire. Polished wire in straight lengths shall be free of decarburization.

Nominal diameter d / mmComplete decarburization depth / mmTotal decarburization depth / mm
d≤7.00≤0.01≤0.10
7.00<d≤15.00≤0.02≤0.15
15.00<d≤25.00≤0.03≤0.25
25.00<d≤32.00≤0.04≤0.32
d>32.00

For d>32.00 mm, permissible decarburization depth is by agreement. Decarburization guarantees for annealed wire shall not automatically be applied to HD wire or grades outside the stated conditions.

6. Inspection, packaging and inspection certificate

Inspection itemSampling quantity and locationTest method
Chemical composition1 coil (or straight length) per heat; GB/T 20066GB/T 4336、223、20123、20125
Tensile testOne end of each of 3 coils (or straight lengths)GB/T 228.1
Upsetting testOne end of each of 3 coils (or straight lengths)YB/T 5293
HardnessOne end of each of 3 coils (or straight lengths)GB/T 230.1
MicrostructureOne end of each of 3 coils (or straight lengths)GB/T 13298、38770
Decarburization depthOne end of each of 3 coils (or straight lengths)GB/T 224
DimensionsEvery coil (or straight length), over its full lengthMeasuring instruments of suitable accuracy
Surface qualityEvery coil (or straight length), over its full lengthVisual inspection

Table 7: when fewer than 3 coils are ordered, sample every coil. Other sampling quantities and locations may be agreed. Referee chemical analysis is in accordance with GB/T 223. Each batch shall have the same heat number, dimensions, heat-treatment condition and delivery condition. Inspection, acceptance, retesting, packaging, marking, storage and inspection certificates are governed by GB/T 2103. Results are evaluated using rounded-value comparison in accordance with GB/T 8170.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — ML20MnA

Basis: GB/T 5953-2026

Chemical composition source: Original standard not yet verified

Original standard not yet verified

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI

Carbon equivalent calculator →