01Applicable standardGB/T 24242.2-2020
02Material gradeC52D
03Product formWire rod for general-purpose wire drawing
04Delivery informationSubject to order specifications

Material technical data

Chemical composition

Cast analysis, mass fraction %. Unspecified values are not zero.

ElementMass fraction / %
C0.5~0.55
Si0.1~0.3
Mn0.5~0.8
P≤0.03
S≤0.025
Cr≤0.15
Ni≤0.2
Mo≤0.05
Cu≤0.25
Al≤0.01

Properties and applicable conditions

Mechanical properties for this grade are agreed between supplier and purchaser and stated in the contract. Recommended variation in Table 2 is not a tensile-strength guarantee.

Standard reference and ordering limitations

  • Cast analysis; composition is expressed as mass fraction, %. An unspecified lower limit is not zero.
  • 4.2.4: Unlisted elements shall not be intentionally added without purchaser consent. Cr and V may be added by agreement at ordering: Cr≤0.30%, V≤0.10%.
  • 4.2.5: For C26D–C92D, agreement may raise the C upper limit by 0.01% or lower the lower limit by 0.01%. This does not expand the default table limits.
  • 4.2.6: The Si lower limit for galvanizing, or the Si upper limit for C4D–C20D, may be separately agreed at ordering.
  • 4.2.8–4.2.10: By agreement, Cu≤0.20%; for C48D–C92D, Cu+Sn≤0.25% may be specified; Al of 0.01%–0.06% with Si≤0.10% may be agreed.
  • 4.3: Mechanical properties of composition-designated grades are agreed between supplier and purchaser. Table 2 gives recommended within-batch tensile-strength variation, not guaranteed tensile-strength limits.
  • Delivery condition, dimensions, surface, packaging and acceptance shall follow GB/T 24242.1—2020 and the order.

Reference: GB/T 24242.2-2020,Table 1. Website information does not replace the official standard, order specifications or material certificates.

Illustrative packaging

Illustrative packaging
Wire-frame packaging · Illustration; packaging is subject to order confirmation.

Product and packaging images are illustrations; they do not identify a heat, stock availability, dimensions or a default delivery method. Confirm product form, delivery condition, packaging and acceptance requirements in the enquiry and order.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Submit a technical enquiry for this material

Contact our technical team →
WhatsApp Technical enquiry →