Products/GB/T 8731-2008

MATERIAL DATA · WIRE ROD

Y45Sn · Free-cutting structural steel wire rod

GB/T 8731—2008. Dimensions, delivery condition, quantity and acceptance requirements are confirmed in the order technical agreement.

Y45Sn Illustrative product image
Y45Sn · Free-cutting structural steel wire rod · Illustrative product image
01Applicable standardGB/T 8731-2008
02Material gradeY45Sn
03Product formFree-cutting structural steel wire rod
04Delivery informationSubject to order specifications

Material technical data

Y45Sn · GB/T 8731-2008

Free-cutting structural steel; hot-rolled bar and wire-rod hardness conditions stated separately · 7.1.1/Table 3 · PDF page 8 · Mass fraction %

ElementHeat analysis / guide composition
C0.4~0.48
Si≤0.4
Mn0.6~1
P0.03~0.07
S≤0.06
Sn0.09~0.25

Verified against the actual original text of GB/T 8731—2008 Table 3; Composition is the heat analysis mass fraction wt%; elements not listed shall not be filled as 0. This standard applies to free-cutting structural steels; Default is UC for machining; UP for pressure processing must be specified in the contract; Supply purpose or cold heading applicability cannot be inferred solely from the grade. Allowable deviations for product analysis of S and Sn are given in Table 5 of 7.1.3; Separated from heat analysis boundaries; other elements follow GB/T 222 and have not been verified item by item. The upper limit of HBW in Table 6 applies only to bars and wire rods delivered in the hot-rolled condition; Mechanical properties for other conditions/products or Annex A require confirmation under the supplier-purchaser agreement and must not be applied automatically. Additional examinations for macrostructure, decarburization and inclusions follow purchaser requirements and the applicable clauses; without agreement, they must not be treated as already performed. The tin-containing grades in Table 3 carry a patent note.; Only chemical compositions listed in the original text of the standard are recorded; no inference of permission or supply is made.

Properties and applicable conditions

ConditionRequirement
Maximum Brinell hardness HBW of hot-rolled bars and wire rod≤241

Original source: GB/T 8731—2008

Illustrative packaging

Illustrative packaging
Illustrative packaging; details are confirmed in the order.

Illustrative company wire products and packaging; the images do not identify the listed grade’s heat or batch, current stock, or default delivery conditions.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.