01Applicable standardJIS G 3506-2024
02Material gradeSWRH27
03Product formHigh-carbon steel wire rod
04Delivery informationSubject to order specifications

Material technical data

SWRH27 · JIS G 3506-2024

High-carbon steel wire rod; see applicable further-processing and delivery-by-agreement conditions · Clause 4/Table 1; Clause 6/Table 2 and note; Annex JA.1 · PDF page 1、5、6、7、11 · Mass fraction %

ElementHeat analysis / guide composition
C0.24~0.31
Si0.15~0.35
Mn0.3~0.6
P≤0.03
S≤0.03

Based on the official Japanese original text of Tables 1/2 and Normative Annex JA of JIS G3506:2024; Heat analysis, mass fraction wt%. Applicable to wire rod intended for further processing into hard-drawn steel wire, oil-quenched and tempered steel wire, prestressed concrete steel wire, galvanized steel strand, steel wire rope, etc.; This standard does not include wire rod for piano wire and wire rod for bridge cables. Cannot be automatically regarded as applicable for cold heading or as a supply guarantee by the company. The default chemical ranges in Table 2 are separate from the narrowed C ranges in JA.1 adopted only by agreement between supplier and purchaser: the upper and lower limits of the agreed range are narrowed inward by 0.01 percentage points each, and are not adopted automatically by default. Alloying elements not listed in Table 2 shall not be intentionally added except for the purpose of finishing steelmaking; Unspecified values shall not be filled as zero, nor shall the complete carbon equivalent be calculated based on this. Clause 9 generally does not specify fixed mechanical properties. Verification shall be performed according to JA.3/JA.4 only when a target tensile strength has been agreed upon and the corresponding agreed delivery condition is adopted; The ±100/±120MPa in Table JA.1 are allowable deviations around the agreed target, not the absolute Rm range, nor a substitute for the target value. Clause 7.1 specifies an average total decarburization layer depth ≤0.20mm; JA.2 may be tightened to ≤0.15mm by agreement. Average total decarburization depth is not the maximum depth of a single field of view; whether to adopt the agreed value must be confirmed separately. Austenitic grain size and non-metallic inclusion limits must be specified by the purchaser and confirmed by agreement under 7.2; a rating cannot be assigned automatically from the grade alone. Table 3 standard diameters are 5.5, 6, 6.4, 7, 8, 9, 9.5, 10, 11, 12, 13, 14, 15mm; Table 4: for diameters ≤15mm, the tolerance is ±0.40mm and the out-of-roundness is ≤0.64mm; For >15mm, agreement is required; do not extrapolate. Inspection, sampling, dimensions, surface, and other product standard conditions shall be verified separately; The relationship with the ISO 16120 series is one of modified adoption, which does not equate to automatic interchangeability of grades.

Original source: JIS G 3506:2024

Historical editions and other standard references

The following editions are separate references and are not the default applicable standards for the products above. Composition and delivery conditions must not be transferred between editions.

SWRH27 · JIS G 3506-2004

High-carbon steel wire rod · Clauses 3 and 4, main-text Table 1, and notes · PDF page 4、5 · Mass fraction %

ElementHeat analysis / guide composition
C0.24~0.31
Si0.15~0.35
Mn0.3~0.6
P≤0.03
S≤0.03
  • Default C range in Table 1 is as above; narrowing of C upper and lower limits by 0.01 percentage points each is adopted only by mutual agreement.
  • 5.1 Average fully decarburized layer depth ≤0.20mm; this inspection may be omitted unless specifically requested by the purchaser.

Original source: JIS G 3506:2004

Illustrative packaging

Illustrative packaging
Illustrative packaging; details are confirmed in the order.

Illustrative company wire products and packaging; the images do not identify the listed grade’s heat or batch, current stock, or default delivery conditions.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Submit a technical enquiry for this material

Contact our technical team →
WhatsApp Technical enquiry →
Image and content use · Creation Group