Products/EN ISO 683-4-2018

MATERIAL DATA · WIRE ROD

36SMn14 · Free-cutting steel wire rod

EN ISO 683-4:2018. Dimensions, delivery condition, quantity and acceptance requirements are confirmed in the order technical agreement.

36SMn14 Illustrative product image
36SMn14 · Free-cutting steel wire rod · Illustrative product image
01Applicable standardEN ISO 683-4-2018
02Material grade36SMn14
03Product formFree-cutting steel wire rod
04Delivery informationSubject to order specifications

Material technical data

36SMn14 · EN ISO 683-4-2018

Free-cutting steel semi-finished products, bars and wire rod; see delivery-state and dimensional conditions · Table 2 and notes a–c; Table 3; 1,6.3,7.1,7.3 · PDF page 1、5、7、10、13、14、15 · Mass fraction %

ElementHeat analysis / guide composition
C0.32~0.39
Si≤0.4
Mn1.3~1.7
P≤0.06
S0.1~0.18

Based on the official EN ISO683-4:2018 text, consulted as DIN EN ISO683-4:2018-09; The European foreword confirms the adoption of ISO683-4:2016 without modification; 2018 is the EN adoption version year, while the adopted ISO version remains 2016. The scope includes semi-finished products, bar products, and wire rod of the free-cutting steels listed in Table 2; Bright bars shall refer separately to ISO683-18; standards for different products shall not be automatically conflated. Table 2 is for heat analysis; Verify Table 3 permissible product-analysis deviations separately only when required at ordering; deviations for the same heat must not exceed both the upper and lower limits in opposite ± directions. Grades containing Pb and grades without Pb shall be recorded separately; dashes shall not be filled as 0. The default low Si value for the non-heat-treated group shall be kept separate from the agreed Si 0.10–0.40% under special oxide guarantees; P shall be selected from a default maximum of 0.11%, an agreed range of 0.06–0.11%, or an agreed maximum of 0.05%; agreed conditions shall not be adopted automatically. Elements not listed shall not be intentionally added without the buyer's consent (except additions needed to finish steelmaking); Additions to improve machinability, such as Ca, Se, and Te, must be agreed upon and reported in the inspection documents; the complete carbon equivalent shall not be calculated based on missing items. Table 1: Untreated +U applies to semi-finished products, bar products, and wire rod; +QT delivery condition applies only to bar products listed in Table 1. Agreed properties for untreated products based on reference samples after heat treatment do not mean that wire rod has been quenched and tempered upon delivery. +U hardness in Tables 4–6 shall be kept separate from the tensile strength used for dispute arbitration; In case of dispute, determination shall be based on tensile strength; properties after quenching and tempering shall not be used to replace the untreated delivery condition. No values are listed for the first and last diameter intervals of +QT for 35SMn20/35SMnPb20 in Table 6; dashes shall not be filled as 0 or extrapolated from adjacent diameters; Parentheses for the first two hardness levels of the 44SMn28 group shall be retained as per the original text; the meaning of parentheses and the guarantee range shall be verified separately. Tensile specimens shall be according to Table 7 and ISO6892-1, with a proportional gauge length L0=5.65√S0; Sampling location, cross-section, inspection lot, and inspection document requirements shall be verified separately. According to 7.3, welding is generally not recommended for high S/P free-cutting steels; Suitability for cold heading or other cold forming must also be confirmed in conjunction with the actual material and agreement; material retrieval does not equal processing suitability or supply guarantee.

Original source: EN ISO 683-4:2018

Historical editions and other standard references

The following editions are separate references and are not the default applicable standards for the products above. Composition and delivery conditions must not be transferred between editions.

36SMn14 · EN 10087-1998

Free-cutting steel semi-finished products, bars and wire rod; delivery state according to the standard and order · Table 1 and footnote a/b · PDF page 1、6 · Mass fraction %

ElementHeat analysis / guide composition
C0.32~0.39
Si≤0.4
Mn1.3~1.7
P≤0.06
S0.1~0.18

Original 1998 edition Table 1 gives cast analysis in mass percent wt%; unlisted elements are not zero. / Permissible product-analysis deviations in Table 2 cannot be added to Table 1 cast-analysis limits. / This standard covers free-cutting steel bars, wire rod and semi-finished products; specific delivery/heat treatment and cold-heading suitability require separate verification.

Original source: EN 10087:1998

Illustrative packaging

Illustrative packaging
Illustrative packaging; details are confirmed in the order.

Illustrative company wire products and packaging; the images do not identify the listed grade’s heat or batch, current stock, or default delivery conditions.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Submit a technical enquiry for this material

Contact our technical team →
WhatsApp Technical enquiry →
Image and content use · Creation Group