Products/BS EN ISO 4957:2018

MATERIAL DATA · TOOL STEEL

70MnMoCr8 · Tool steel

BS EN ISO 4957:2018 · Table 4 and notes a–g. Select for cold-work, hot-work or high-speed tool-steel applications. Intended use and product form require confirmation in the technical agreement.

70MnMoCr8 Illustrative product image
70MnMoCr8 · Tool steel (product form subject to the order) · Illustrative product image
01Applicable standardBS EN ISO 4957:2018
02Material grade70MnMoCr8
03Product formTool steel (product form subject to the order)
04Delivery informationSubject to order specifications

Material technical data

Chemical composition

Cast analysis, mass fraction %. Unspecified values are not zero.

ElementMass fraction / %
C0.65~0.75
Si0.1~0.5
Mn1.8~2.5
Cr0.9~1.2
Mo0.9~1.4
P≤0.03
S≤0.03

Properties and applicable conditions

PropertyStandard requirements and applicable conditions
Annealed hardness HBW / maximum248
Hardening testAustenitizing 835±10 °C ; air quenching ; tempering 180±10 °C ; hardness≥58 HRC

Standard reference and ordering limitations

  • Cast analysis, mass fraction %. A dash means the standard gives no separate requirement; it does not mean zero.
  • Unlisted elements shall not be intentionally added without purchaser consent, except additions needed to finish steelmaking.
  • Permissible product-analysis deviations do not expand the default cast-analysis limits.
  • Tool-steel classification and hardness depend on application, heat treatment and test conditions; they do not establish cold-heading suitability or guarantee properties in an arbitrary condition.
  • Table 4: alloy cold-work tool steels; cast analysis, wt%; default P and S each ≤.030%.
  • Product-analysis deviations in Table 5 must not be applied to the default cast-analysis limits.
  • Unlisted elements shall not be intentionally added without purchaser consent, except to finish steelmaking. Dashes are not entered as zero.
  • Annealed and cold-drawn (+A+C) hardness may be 20 HBW higher than annealed (+A) hardness. Hardness values for different conditions must not be interchanged.

Reference: BS EN ISO 4957:2018,Table 4 and notes a–g. Website information does not replace the official standard, order specifications or material certificates.

Illustrative packaging

Illustrative packaging
Pallet packaging · Illustration; packaging is subject to order confirmation.

Product and packaging images are illustrations; they do not identify a heat, stock availability, dimensions or a default delivery method. Confirm product form, delivery condition, packaging and acceptance requirements in the enquiry and order.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Submit a technical enquiry for this material

Contact our technical team →