Products/Q/BQB 517-2023

MATERIAL DATA · COLD FORMING

40CrMo Steel Material for Cold Forming (Wire Rod)

40CrMo · Q/BQB 517-2023. Delivery condition, dimensions, mechanical properties, hardenability and acceptance must be confirmed against the applicable standard and order agreement. Similar grades are not interchangeable; this page does not guarantee supply or forming performance.

40CrMo Steel Material for Cold Forming (Wire Rod) product image
40CrMo · Cold forming wire rod
01Applicable standardQ/BQB 517-2023
02Material grade40CrMo
03Product formCold forming wire rod
04Delivery informationTo be confirmed against the order technical requirements

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

Standard and grade references

Baosteel agreement / special grade: a national or international standard designation for this complete name has not been confirmed. Approximate cross-references are not equivalence.

Baosteel delivery specification: Q/BQB 517-2023

The values below come from the identified Baosteel standard or agreement, not from a general national-standard chemistry table. Different sources are shown separately and their limits are not combined.

Chemical composition (mass fraction, %)

Q/BQB 517-2023 · PDF 14 · Table 2 · Row 34

CSiMnPSCrMoBAltOther
0.38-0.43≤0.150.60-0.90≤0.020≤0.0200.90-1.200.15-0.30≤0.00500.02-0.05Ni:≤0.25Cu:≤0.12V:≤0.10

Delivery condition, dimensions, mechanical properties, hardenability and acceptance must be confirmed against the applicable standard and order agreement. Similar grades are not interchangeable; this page does not guarantee supply or forming performance.

Illustrative product photograph randomly selected from company photos; it does not identify this grade, heat or batch.

Application and ordering note

Chemical composition, mechanical properties, delivery condition and other technical requirements are subject to the currently applicable standard edition, customer drawings and the order technical agreement. Website information does not replace formal quality certification documents.

What to include in the enquiry

Carbon equivalent calculator — 40CrMo

Basis: Q/BQB 517-2023

Chemical composition source: Original standard not yet verified

Original standard not yet verified

A stated upper limit means 0 to that limit. A lower limit alone does not define an upper bound. Missing elements are unknown, not zero. Standard-limit combinations are not measured heat results.

Carbon equivalent supports weldability assessment; it does not approve cold heading, fastener strength or a welding procedure. These formulas do not directly apply to stainless steels, cast irons or non-ferrous metals.

Method reference: TWI