B5 (steel)

3 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for B5 (steel) →

B5 · ASTM A193/A193M-2001

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≥ 0.1 (upper limit not stated)
Cr4 ~ 6
Mn≤ 1 (lower limit not stated)
Mo0.4 ~ 0.65
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

B5 · BS 3100-1991

Original-source verification is incomplete; this is not a formal standard reference

Material category
Alloy steel
Subcategory
Cast steels
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C≤ 0.2 (lower limit not stated)
Cr4 ~ 6
Mn0.4 ~ 0.7
Mo0.45 ~ 0.65
P≤ 0.04 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si≤ 0.75 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

B5 · ASTM A193/A193M-26

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results.

Material category
Alloy steel
Material form
Bolting material for high-temperature or high-pressure service
Standard edition
ASTM A193/A193M-26
Table / clause
Table 1 and applicable footnotes A, B, E, F, G
PDF page references
3、5
Unit
Mass fraction (wt%)
Analysis type
Heat analysis

Carbon-equivalent reference

The composition inputs and formula applicability for A193 carbon-equivalent calculations have not been specifically verified; no calculation is provided.

Composition

ElementComposition requirement
C≥ 0.1 (upper limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Cr4.0 ~ 6.0
Mo0.4 ~ 0.65

Applicable conditions and limitations

ASTM A193/A193M-26, Table 1: heat-analysis mass fractions in wt%; single values are maxima unless a range or minimum is stated. Ellipses indicate no requirement and are not entered as zero.

Intentional additions of Bi, Se, Te and Pb are prohibited; this does not mean that measured contents of these elements are zero.

Product-analysis tolerances in Table 1 are applied separately and are not added in advance to the heat-analysis ranges.

Only chemical composition has been checked in this record. Class, heat treatment, dimensions and inch-pound or metric properties require separate confirmation. This is not a guarantee of cold-heading suitability, finished-product properties or actual supply.