Products/GB/T 28906

MATERIAL DATA · COLD FORMING

MFT9DP Alambre para estampación en frío | Creation Group

Grado según GB/T 5953. El estado de suministro, las dimensiones, las propiedades mecánicas y la aceptación se confirman mediante contrato, pedido y plano.

01StandardGB/T 28906
02GradeMFT9DP cold-heading steel丝 | Creation Group
03Product formCold heading wire
04Delivery noteConfirmed by order specification

Material technical data

Only data directly related to this material is shown here. Inspection, equipment, process and packaging information is linked separately.

Enquire this grade

Material technical data

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

Application and ordering note

Chemical composition, mechanical properties, tolerances and delivery condition must be confirmed against the applicable standard edition, customer drawing and order specification.

What to include in the enquiry

Send a technical enquiry

Contact technical team →
WhatsApp Technical enquiry →