ZTSCM435
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for ZTSCM435 →Material demand assessment
Looking for ZTSCM435 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
ZTSCM435 · Q/320412 ZTG 223—2021
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Cold-heading steel
- Subcategory
- Cold-heading steel
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- 2021 edition; Published and implemented 2021-05-18; Supersedes 2020 edition
- Document title
- Hot-rolled cold-heading steel wire rod for automotive fasteners
- Table / clause
- Table 1
- PDF page references
- 4
- Unit
- Mass fraction (wt%)
- Manufacturer
- Zenith Steel Group Co., Ltd.
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.33 ~ 0.38 |
| Si | 0.15 ~ 0.35 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cr | 0.9 ~ 1.2 |
| Mo | 0.15 ~ 0.3 |
| Al | ≥ 0.02 (upper limit not stated) |
| Ni | ≤ 0.2 (lower limit not stated) |
| Cu | ≤ 0.2 (lower limit not stated) |
Applicability and limitations
Zhongtian Steel Q/320412 ZTG 223—2021, Table 1, row 7, PDF page 4, cast analysis wt%. Applies to hot-rolled wire rod; specific orders, delivery and supply by Creation Group require separate confirmation.
Composition conditions
- Table 1 heat analysis, mass fractions wt%; Upper limits for residual Cr, Ni, Cu, and Mo for Group I shall be supplemented according to Table 3, with priority given to specific provisions within the table.
- Applicable to hot-rolled round wire rod of Φ5.5–25.0mm for automotive fasteners; Wire rod is delivered in the hot-rolled condition.
- A horizontal line indicates that the limit is not listed in the table, which does not equal zero; Measured mechanical-property data in the hot-rolled condition are to be reported for information only; they are not general guaranteed values.