ZT10B21

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for ZT10B21 →

Material demand assessment

Looking for ZT10B21 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

ZT10B21 · Q/320412 ZTG 223—2021

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Cold-heading steel
Subcategory
Cold-heading steel
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
2021 edition; Published and implemented 2021-05-18; Supersedes 2020 edition
Document title
Hot-rolled cold-heading steel wire rod for automotive fasteners
Table / clause
Table 1
PDF page references
4
Unit
Mass fraction (wt%)
Manufacturer
Zenith Steel Group Co., Ltd.

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.3167–0.5033Known-element contribution; incomplete value; missing V CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2240–0.3358Known-element contribution; incomplete value; missing V Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2550–0.3700 Envelope of independent element limits from manufacturer data; neither standard guarantee values nor measured heat results CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.18 ~ 0.23
Si≤ 0.1 (lower limit not stated)
Mn0.7 ~ 1.0
P≤ 0.025 (lower limit not stated)
S≤ 0.025 (lower limit not stated)
Cr0.1 ~ 0.3
Al≥ 0.02 (upper limit not stated)
Ti≥ 0.02 (upper limit not stated)
B0.0008 ~ 0.0035
Ni≤ 0.2 (lower limit not stated)
Cu≤ 0.2 (lower limit not stated)
Mo≤ 0.1 (lower limit not stated)

Applicability and limitations

Zhongtian Steel Q/320412 ZTG 223—2021, Table 1, row 4, PDF page 4, cast analysis wt%. Applies to hot-rolled wire rod; specific orders, delivery and supply by Creation Group require separate confirmation.

Composition conditions

Verification notes

Both grade tables and residual-element groups in the publicly available 2021 edition were checked row by row; Verification excludes the watermark color layer in the PDF source document.