← BackMaterial grade directory

ZGMN13-4

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for ZGMN13-4 →

Material demand assessment

Looking for ZGMN13-4 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

ZGMn13-4 · JB /T 6404-1992

Original-source verification is incomplete; this is not a formal standard reference

Material category
Cast steels
Subcategory
Cast steels
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C0.9 ~ 1.2
Mn11 ~ 14
P≤ 0.07 (lower limit not stated)
S≤ 0.05 (lower limit not stated)
Si0.3 ~ 0.8

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

ZGMn13-4 · YB /T 036.4-1992

Original-source verification is incomplete; this is not a formal standard reference

Material category
Cast steels
Subcategory
Cast steels
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: composition source not verified; standard-range carbon equivalent is not calculated
Pcm (Ito–Bessyo): composition source not verified; standard-range carbon equivalent is not calculated
CET: composition source not verified; standard-range carbon equivalent is not calculated

Composition

ElementComposition requirement
C0.9 ~ 1.2
Mn11 ~ 14
P≤ 0.07 (lower limit not stated)
S≤ 0.04 (lower limit not stated)
Si0.3 ~ 0.6

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →