← BackMaterial grade directory

Y10CR17

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for Y10CR17 →

Material demand assessment

Looking for Y10CR17 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

Y10Cr17 · GB /T 20878-2007

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Ferritic stainless and heat-resistant steels
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 20878—2007
Table / clause
Table 3, No. 86
PDF page references
11
Unit
Mass fraction (wt%)
Analysis type
Standard composition requirements

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Si≤ 1 (lower limit not stated)
Mn≤ 1.25 (lower limit not stated)
P≤ 0.06 (lower limit not stated)
S≥ 0.15 (upper limit not stated)
Ni≤ 0.6 (lower limit not stated)
Cr16 ~ 18
Mo≤ 0.6 (lower limit not stated)

Applicability and limitations

Original GB/T 20878—2007 composition, mass fractions wt%; Values in parentheses are maximum permitted additions. S ≥0.15; Ni (0.60) and Mo (0.60) are maximum permitted additions. This standard does not guarantee cold-heading suitability or actual supply. GB/T 20878—2007 is a historical edition; This record does not replace verification of the current standard, contract or material applicability.

Verification notes

GB/T 20878—2007 historical original, Table 3, entry 86. The complete 45-page scan was checked. The standard is withdrawn; the historical edition’s application limits are retained.