XM-19
5 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for XM-19 →Material demand assessment
Looking for XM-19 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
XM-19 · ASTM A358/A358M-2024
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Welded-pipe reference
- Original record status
- Historically referenced table verified
- Standard edition
- ASTM A240/A240M-2014
- Table / clause
- Table 1 and footnotes A–O
- PDF page references
- 1、2、6
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.06 (lower limit not stated) |
| Mn | 4.0 ~ 6.0 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 0.75 (lower limit not stated) |
| Cr | 20.5 ~ 23.5 |
| Ni | 11.5 ~ 13.5 |
| Mo | 1.5 ~ 3.0 |
| N | 0.2 ~ 0.4 |
| Nb | 0.1 ~ 0.3 |
| V | 0.1 ~ 0.3 |
Applicability and limitations
The chemical composition currently uses only the verified base-material ranges in the original ASTM A240/A240M—2014; The applicable composition-standard edition and full requirements for A358—2024 have not been verified; compliance with a newer edition cannot be confirmed on this basis. Clause 6.1.1 of A358—2024 references A240/A240M base material; Clause 7.2 specifies separate requirements for welding filler metal; No weld-metal or mixed whole-tube composition is currently provided. Class 1 are welding and radiographic examination classes, not separate chemical-composition grades; This record does not establish capability to supply welded tube; a linked wire-rod product does not establish direct supply of A358 welded tube. Table 1 gives heat-analysis mass percentages; A single value without a stated range or minimum is a maximum; unspecified elements are not entered as zero. Cb and Nb are the same element; Where both a formula and a fixed limit apply, the stricter limit is used. This is a plate, sheet and strip standard; cold-heading wire applications and actual supply require separate verification. Clause 4.1 also requires compliance with the applicable provisions of ASTM A480/A480M; This record displays the heat composition in Table 1; it does not establish verification of A480 or all product acceptance requirements. Other elements in the original table: Cb 0.10–0.30 V 0.10–0.30; See the limits below for the specific coupled requirements.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
Historical base-material reference: ASTM A240/A240M—2014; Weld metal and the applicable A358—2024 edition have not been verifiedXM-19 · ASTM A 276-2006
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.06 (lower limit not stated) |
| Cr | 20.5 ~ 23.5 |
| Mn | 4 ~ 6 |
| Mo | 1.5 ~ 3 |
| N | 0.2 ~ 0.4 |
| Ni | 11.5 ~ 13.5 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| V | 0.1 ~ 0.3 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
XM-19 · ASTM A 314-2025
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.06 (lower limit not stated) |
| Cr | 20.5 ~ 23.5 |
| Mn | 4 ~ 6 |
| Mo | 1.5 ~ 3 |
| N | 0.2 ~ 0.4 |
| Nb | 0.1 ~ 0.3 |
| Ni | 11.5 ~ 13.5 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| V | 0.1 ~ 0.3 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
XM-19 · ASTM A580/A580M-2018
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.06 (lower limit not stated) |
| Cr | 20.5 ~ 23.5 |
| Mn | 4 ~ 6 |
| Mo | 1.5 ~ 3 |
| N | 0.2 ~ 0.4 |
| Nb | 0.1 ~ 0.3 |
| Ni | 11.5 ~ 13.5 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| V | 0.1 ~ 0.3 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
XM-19 · ASTM A580/A580M-2023
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.06 (lower limit not stated) |
| Cr | 20.5 ~ 23.5 |
| Mn | 4 ~ 6 |
| Mo | 1.5 ~ 3 |
| N | 0.2 ~ 0.4 |
| Nb | 0.1 ~ 0.3 |
| Ni | 11.5 ~ 13.5 |
| P | ≤ 0.04 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | ≤ 1 (lower limit not stated) |
| V | 0.1 ~ 0.3 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.