X8NI9
2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for X8NI9 →Material demand assessment
Looking for X8NI9 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
X8Ni9 · EN 10269-2013
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10269-2013
- Table / clause
- Table1 quenched-and-tempered steels and note a/b/c
- PDF page references
- 17、19
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | ≤ 0.35 (lower limit not stated) |
| Mn | 0.3 ~ 0.8 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
| Ni | 8.5 ~ 10.0 |
| V | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
EN10269:2013 Table 1, section on steels for quenching and tempering; official BS adoption in English, PDF17 and footnotes PDF19; heat analysis wt%.. ; The Al column is total aluminum; For ≥.020 without a specified upper limit, only the lower limit is retained; no upper limit shall be created. ; Note b sulfur agreement applies only to grades with Note b; 27NiCrMoV15-6 magnetic properties Note c carbon upper limit .28 selected separately. ; Elements not listed shall not be intentionally added without the consent of the purchaser, except additions needed to finish steelmaking; Blank does not represent zero. ; Product analysis deviation, mechanical properties, heat treatment, and cold-heading supply suitability shall be verified separately, and not automatically added to the product center.
Verification notes
Quenched-and-tempered steels in official English Table 1 and the applicable footnotes were visually checkedX8Ni9 · NF EN 10269:1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Alloy steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Original record status
- Original-standard record
- Standard edition
- NF EN 10269:1999
- Table / clause
- EN 10269:1999 Table 1 and footnotes 1 and 2
- PDF page references
- 2、22、23
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.1 (lower limit not stated) |
| Si | ≤ 0.35 (lower limit not stated) |
| Mn | 0.3 ~ 0.8 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
| Mo | ≤ 0.1 (lower limit not stated) |
| Ni | 8.5 ~ 10.0 |
| V | ≤ 0.05 (lower limit not stated) |
Applicability and limitations
The cover of NF EN 10269:1999 explicitly adopts EN 10269:1999; Preserve the correspondence between the French adoption version and the European version; do not label as other countries or new editions. ; Table 1 gives heat-analysis mass percentages; Single values in P and S columns are upper limits; other single values are parsed according to the inequality signs in the original table; Unspecified elements shall not be filled as zero. ; Applies to billets, bars and wire rod of steels and nickel alloys for fasteners with specified high- or low-temperature properties.; Cold heading and actual supply must be verified in conjunction with delivery condition, dimensions, and process. ; Table 1 Footnote 1: Elements not listed in the table shall not be intentionally added without the buyer's consent (except additions needed to finish steelmaking); Elements that affect properties must be prevented from being introduced via scrap steel, etc.. ; This record only verifies the heat analysis composition in Table 1; product analysis tolerances in Table 2 shall not be automatically added to the heat limits.
Combined limits
- Combined-element limits