X6NICRNBCE 32-27

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X6NICRNBCE 32-27 →

Material demand assessment

Looking for X6NICRNBCE 32-27 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X6NiCrNbCe 32-27 · DIN EN 10095-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10095:2018-12
Table / clause
Table 2, footnotes 1/*; 7.2
PDF page references
1、2、3、9、16

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Si≤ 0.3 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.01 (lower limit not stated)
Cr26.0 ~ 28.0
Ni31.0 ~ 33.0
N≤ 0.11 (lower limit not stated)
Al≤ 0.025 (lower limit not stated)
Ce0.05 ~ 0.1
Nb0.6 ~ 1.0

Applicability and limitations

DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply.

Combined limits

Combined-element limits
    Elements requiring measured values from the same heat

      Verification notes

      Official original DIN EN 10095:2018-12 composition and footnotes have been checked; Spacing within grade designations is normalized for correspondence; the EN year and DIN correction date are retained separately.
      WhatsApp Technical enquiry →