X6CRNI25-20

7 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X6CRNI25-20 →

Material demand assessment

Looking for X6CRNI25-20 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X6CrNi25-20 · EN 10028-7-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Cr24 ~ 26
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni19 ~ 22
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X6CrNi25-20 · EN 10272-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Cr24 ~ 26
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni19 ~ 22
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X6CrNi25-20 · NF EN 10028-7-2000

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Cr24 ~ 26
Mn≤ 2 (lower limit not stated)
N≤ 0.11 (lower limit not stated)
Ni19 ~ 22
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X6CrNi25-20 · NF EN 10028-7-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Cr24 ~ 26
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni19 ~ 22
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X6CrNi25-20 · NF EN 10088-1-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Cr24 ~ 26
Mn≤ 2 (lower limit not stated)
N≤ 0.11 (lower limit not stated)
Ni19 ~ 22
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X6CrNi25-20 · ISO 15510-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.1
Cr24 ~ 26
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni19 ~ 22
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X6CrNi25-20 · ISO 9328-7-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C0.04 ~ 0.08
Cr24 ~ 26
Mn≤ 2 (lower limit not stated)
N≤ 0.1 (lower limit not stated)
Ni19 ~ 22
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →