X5CRNIMOTI15-2

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X5CRNIMOTI15-2 →

Material demand assessment

Looking for X5CRNIMOTI15-2 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X5CrNiMoTi15-2 · EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 2 and notes a–c; all 21 ferritic stainless steel grades
PDF page references
1、3、7、8

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr13.5 ~ 15.5
Mo0.2 ~ 1.2
Ni1.0 ~ 2.5
Ti0.3 ~ 0.5

Applicability and limitations

EN10088-1:2005, Table 2, cast/heat-analysis mass fractions wt%; complete Table 2 in the official SIST adoption preview PDF8; The preview is not the complete standard. ; Note a: unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; A blank is not zero; no residual maximum is inserted without a source. ; Note b applies only to grades marked b; S must be checked separately for the selected product and property conditions and is not extended to the entire table. ; The coupled minimum for Ti/Nb/Zr and C/N is retained separately; no N maximum is provided in the table, and this is not entered as zero; The corresponding coupled condition cannot be confirmed without measured N. ; This part is a stainless steel designation list; specific delivery and mechanical-property requirements must follow the corresponding product standard; Cold-heading suitability, supply or equivalence between national editions is not established.

Combined limits

Elements requiring measured values from the same heat

    Verification notes

    Visual verification of all 21 rows and footnotes in original Table 2; stabilization is retained only for explicitly specified routes.