← BackMaterial grade directory

X5CRNIMO 17-12-2

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X5CRNIMO 17-12-2 →

Material demand assessment

Looking for X5CRNIMO 17-12-2 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X5CrNiMo 17-12-2 · DIN EN 10263-5-2002

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10263-5-2002
Table / clause
Table 2 and notes a–e; Table 3 is cited only for deviations
PDF page references
1、8、9

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.5 ~ 18.5
Mo2.0 ~ 2.5
Ni10.0 ~ 13.0
N≤ 0.11 (lower limit not stated)
Cu≤ 1.0 (lower limit not stated)

Applicability and limitations

The original webpage states DIN EN 10263-5-2018; The composition in this record was actually verified against DIN EN 10263-5-2002; the edition is now identified as 2002 according to the original evidence; See the separate complete-table record for edition 2018. ; Source actually used: DIN EN10263-5:2002-02, the German-language adoption of EN10263-5:2001; PDF8, Table 2 and notes a–e. ; Default heat analysis in wt%.; Apply product-analysis tolerances in Table 3 separately; do not add them to the default heat-analysis range. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish steelmaking; Residual elements must not impair the properties or intended use. ; The older table does not use the 2017 edition’s separate sulfur conditions; do not copy machining/welding/polishing options from the newer edition.. ; For Ti-stabilized grades, check 5×C≤Ti≤0.70% against measured C.; Does not apply to grades for which Ti is not specified. ; Standard range for cold-heading and cold-extrusion; actual supply, dimensions, delivery condition, and performance still require confirmation..

Original condition-branch records

Default heat-analysis values in historical Table 2

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.5 ~ 18.5
Mo2.0 ~ 2.5
Ni10.0 ~ 13.0
N≤ 0.11 (lower limit not stated)
Cu≤ 1.0 (lower limit not stated)

Verification notes

The original webpage states DIN EN 10263-5-2018; The composition in this record was actually verified against DIN EN 10263-5-2002; the edition is now identified as 2002 according to the original evidence; See the separate complete-table record for edition 2018.

X5CrNiMo 17-12-2 · DIN EN 10269-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Composition basis in the adopted standard verified
Standard edition
EN 10269-2013
Table / clause
Table 1 and notes a–c

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default sulfur content in Table 1
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
S 0.015–0.030% agreed at enquiry or ordering to improve machinability
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Weldability condition S 0.008–0.030% agreed at enquiry or ordering
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr16.5 ~ 18.5
Mo2.0 ~ 2.5
Ni10.0 ~ 13.0
N≤ 0.1 (lower limit not stated)

Applicability and limitations

DIN EN 10269:2014-02 adopts EN 10269:2013; Composition in this record follows EN 10269:2013, Table 1 and footnotes; the actual text read is the official BS adoption. Heat-analysis mass fractions wt%; Product-analysis tolerances require separate verification under Table 2. ; The agreed sulfur condition in Table 1, note b applies only to grades marked b; default, machining and welding ranges are retained separately. ; This standard covers steels and nickel alloys for high- and low-temperature fasteners; cold-heading suitability is not established for every grade or delivery condition. ; Unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish steelmaking; Unspecified values are not treated as zero.

Original condition-branch records

Default sulfur content in Table 1

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr16.5 ~ 18.5
Mo2.0 ~ 2.5
Ni10.0 ~ 13.0
N≤ 0.1 (lower limit not stated)

S 0.015–0.030% agreed at enquiry or ordering to improve machinability

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S0.015 ~ 0.03
Cr16.5 ~ 18.5
Mo2.0 ~ 2.5
Ni10.0 ~ 13.0
N≤ 0.1 (lower limit not stated)

Weldability condition S 0.008–0.030% agreed at enquiry or ordering

ElementComposition requirement
C≤ 0.07 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S0.008 ~ 0.03
Cr16.5 ~ 18.5
Mo2.0 ~ 2.5
Ni10.0 ~ 13.0
N≤ 0.1 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

The adoption relationship and original composition in the corresponding EN, Table 1 have been checked; The complete main text of DIN has not been checked page by page
WhatsApp Technical enquiry →