← BackMaterial grade directory

X2NICRALTI32-20

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X2NICRALTI32-20 →

Material demand assessment

Looking for X2NICRALTI32-20 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X2NiCrAlTi32-20 · EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 4 and continuation; notes a–e; all 50 austenitic corrosion-resistant steel grades
PDF page references
1、3、11、12

Source document

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Default sulphur requirement; default Ni; note c: Cu≤1.0% for cold heading/cold extrusion.
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr20.0 ~ 23.0
Ni32.0 ~ 35.0
Al0.15 ~ 0.45
Ti≤ 0.6 (lower limit not stated)

Applicability and limitations

EN 10088-1:2005 Table 4 and continuation: ladle analysis (wt%); the official SIST adoption preview PDF, pages 11/12, covers all 50 grades and notes. Note a: unlisted elements are not intentionally added without purchaser consent, except as needed to complete steelmaking; a blank is not zero. Note b: for grades marked b only, S is selected separately for long products and by property requirement. Note d: the increased Ni maximum for special reasons applies only to listed grades, not all grades. Note c: Cu up to 1.0% for cold heading/extrusion; this condition path is provided here only for grades with blank Cu in the original table. Existing Cu alloy ranges retain their original values; the exception has not automatically rewritten them. The linked Ti≥5C/Nb≥10C and Ti≥8(C+N) conditions are retained; an unlisted N maximum is not zero. Note e: the source warns of skin-contact regulatory issues for high-sulfur free-machining steel; this is retained as a historical warning only and is not a claim of current compliance based on the 2005 text. Listed chemistry and the cold-heading Cu exception alone do not establish overall cold-heading performance or company supply; mechanical and product standards must be checked separately, and national adoption does not mean automatic equivalence.

Combined limits

Combined-element limits
  • Element coefficient
    Ti
    1
    C
    -8
    N
    -8
    Lower limit
    0
    Requirement
    Ti≥8(C+N)
Elements requiring measured values from the same heat
  • N

Original condition-branch records

Default sulfur requirement; default Ni; the cold-heading Cu exception is not selected, so the original-table Cu requirement applies.

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr20.0 ~ 23.0
Ni32.0 ~ 35.0
Al0.15 ~ 0.45
Ti≤ 0.6 (lower limit not stated)

Default sulphur requirement; default Ni; note c: Cu≤1.0% for cold heading/cold extrusion.

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr20.0 ~ 23.0
Ni32.0 ~ 35.0
Al0.15 ~ 0.45
Ti≤ 0.6 (lower limit not stated)
Cu≤ 1.0 (lower limit not stated)

A condition branch must be selected

Yes

Verification notes

Official source Table 4, all 50 rows and footnotes visually checked; conditional route for Cu cells left blank in the original.

X2NiCrAlTi32-20 · ISO 15510-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Al0.15 ~ 0.45
C≤ 0.03 (lower limit not stated)
Cr20 ~ 23
Mn≤ 1 (lower limit not stated)
Ni32 ~ 35
P≤ 0.02 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →