← BackMaterial grade directory

X2CRNIMOV13-5-2

4 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X2CRNIMOV13-5-2 →

Material demand assessment

Looking for X2CRNIMOV13-5-2 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X2CrNiMoV13-5-2 · EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 3 and continuation, notes a–d; all 30 martensitic and precipitation-hardening corrosion-resistant steel grades
PDF page references
1、3、9、10

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Mn≤ 0.5 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr11.5 ~ 13.5
Mo1.5 ~ 2.5
Ni4.5 ~ 6.5
Ti≤ 0.01 (lower limit not stated)
V0.1 ~ 0.5

Applicability and limitations

EN10088-1:2005, Table 3 including its continuation, heat analysis wt%; official English SIST adoption preview PDF9/10. ; Note a: unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; blanks are not filled with zero or a general residual maximum. ; Note b distinguishes sulfur conditions for long products, machining, welding and polishing only for grades marked b; it is not extended to all grades. ; Note c: a narrower C range may be agreed at enquiry and ordering; Without a contract, the original table range is not replaced. ; Note d: only for X7CrNiAl17-7 to improve cold-deformation performance, the Ni maximum is 8.3%; select separately from default 7.8. ; A designation-list standard does not independently establish cold-heading suitability, mechanical-property delivery requirements or product supply; Adopted editions such as NF/DIN are not automatically verified by this European main text.

Verification notes

All 30 rows of Table 3 and footnotes visually checked.

X2CrNiMoV13-5-2 · NF EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Original record status
Composition basis in the adopted standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 3 and continuation, notes a–d; all 30 martensitic and precipitation-hardening corrosion-resistant steel grades
PDF page references
1、3、9、10

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Mn≤ 0.5 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr11.5 ~ 13.5
Mo1.5 ~ 2.5
Ni4.5 ~ 6.5
Ti≤ 0.01 (lower limit not stated)
V0.1 ~ 0.5

Applicability and limitations

NF EN 10088-1:2005 adopts EN 10088-1:2005 (EN 10088-1-2005); See the data basis for the actual composition source file and table number. EN10088-1:2005, Table 3 including its continuation, heat analysis wt%; official English SIST adoption preview PDF9/10. ; Note a: unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; blanks are not filled with zero or a general residual maximum. ; Note b distinguishes sulfur conditions for long products, machining, welding and polishing only for grades marked b; it is not extended to all grades. ; Note c: a narrower C range may be agreed at enquiry and ordering; Without a contract, the original table range is not replaced. ; Note d: only for X7CrNiAl17-7 to improve cold-deformation performance, the Ni maximum is 8.3%; select separately from default 7.8. ; A designation-list standard does not independently establish cold-heading suitability, mechanical-property delivery requirements or product supply; Adopted editions such as NF/DIN are not automatically verified by this European main text.

Verification notes

The formal adoption relationship and corresponding EN composition original have been checked; the complete national adoption text has not been verified page by page.

X2CrNiMoV13-5-2 · EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 3 and continuation, notes a–d; all 30 martensitic and precipitation-hardening corrosion-resistant steel grades
PDF page references
1、3、9、10

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Mn≤ 0.5 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr11.5 ~ 13.5
Mo1.5 ~ 2.5
Ni4.5 ~ 6.5
Ti≤ 0.01 (lower limit not stated)
V0.1 ~ 0.5

Applicability and limitations

EN10088-1:2005, Table 3 including its continuation, heat analysis wt%; official English SIST adoption preview PDF9/10. ; Note a: unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; blanks are not filled with zero or a general residual maximum. ; Note b distinguishes sulfur conditions for long products, machining, welding and polishing only for grades marked b; it is not extended to all grades. ; Note c: a narrower C range may be agreed at enquiry and ordering; Without a contract, the original table range is not replaced. ; Note d: only for X7CrNiAl17-7 to improve cold-deformation performance, the Ni maximum is 8.3%; select separately from default 7.8. ; A designation-list standard does not independently establish cold-heading suitability, mechanical-property delivery requirements or product supply; Adopted editions such as NF/DIN are not automatically verified by this European main text.

Verification notes

All 30 rows of Table 3 and footnotes visually checked.

X2CrNiMoV13-5-2 · ISO 15510-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Martensitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr11.5 ~ 13.5
Mn≤ 0.5 (lower limit not stated)
Mo1.5 ~ 2.5
Ni4.5 ~ 6.5
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.5 (lower limit not stated)
Ti≤ 0.01 (lower limit not stated)
V0.1 ~ 0.5

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →