X2CRNIMON17-12-3

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X2CRNIMON17-12-3 →

Material demand assessment

Looking for X2CRNIMON17-12-3 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X2CrNiMoN17-12-3 · ISO 15510-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
ISO 15510-2014
Table / clause
The current grade row in Table1; Note a and corresponding footnotes (original text on the publishing platform)
PDF page references
10

Source document

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Base range in Table 1
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category
Note c: only where ferrite content must be reduced for a special reason, the Ni maximum may be increased by 1.00 percentage points; This condition must be confirmed
IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.5 ~ 18.5
Mo2.5 ~ 3.0
Ni10.5 ~ 13.0
N0.12 ~ 0.22

Applicability and limitations

ISO 15510:2014, Table 1 gives heat analysis, mass fractions wt%; Under note a, values without a stated range or minimum are maxima; a dash is not treated as zero. Composition rows follow an excerpt of the official PDF edition; relevant footnotes follow the original Table 1 in the Sample text section of the standards publishing platform; Verification of the complete standard text or mechanical properties is not claimed. The standard covers material for wrought products, including ingots and semi-finished products; Similar composition does not establish direct substitution; cold-heading suitability and supply condition require separate confirmation. The S 0.015–0.030% machinability recommendations, 0.008–0.020% weldability recommendation and S≤0.015% polishability recommendation in note b concern specific properties and do not directly replace this row’s sulfur limits. Note c applies only where ferrite content must be reduced for special reasons such as hot workability or low magnetic permeability; The increased Ni maximum is not treated as an unconditional range.

Original condition-branch records

Base range in Table 1

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.5 ~ 18.5
Mo2.5 ~ 3.0
Ni10.5 ~ 13.0
N0.12 ~ 0.22

Note c: only where ferrite content must be reduced for a special reason, the Ni maximum may be increased by 1.00 percentage points; This condition must be confirmed

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.5 ~ 18.5
Mo2.5 ~ 3.0
Ni10.5 ~ 14.0
N0.12 ~ 0.22

A condition branch must be selected

Yes

Verification notes

The row for this grade in Table 1 has been checked against the official PDF; Relevant original footnotes are retained in the supporting verification record; Full standard text and mechanical properties to be verified separately

X2CrNiMoN17-12-3 · ISO TS 15510-2003

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Austenitic stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr16.5 ~ 18.5
Mn≤ 2 (lower limit not stated)
Mo2.5 ~ 3
N0.12 ~ 0.22
P≤ 0.045 (lower limit not stated)
Si≤ 1 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.