← BackMaterial grade directory

X2CRNIMOCUN25-6-3

14 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X2CRNIMOCUN25-6-3 →

Material demand assessment

Looking for X2CRNIMOCUN25-6-3 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X2CrNiMoCuN25-6-3 · NF EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Original record status
Composition basis in the adopted standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 5, note a/b/c and asterisks, covering all 9 duplex corrosion-resistant steel grades
PDF page references
1、3、13

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
N0.2 ~ 0.3
Cr24.0 ~ 26.0
Cu1.0 ~ 2.5
Mo3.0 ~ 4.0
Ni6.0 ~ 8.0

Applicability and limitations

NF EN 10088-1:2005 adopts EN 10088-1:2005; Composition is taken from the original EN table for the same designation. EN10088-1:2005 Table 5 duplex (austenitic-ferritic) corrosion-resistant stainless steels, heat analysis wt%; Official SIST adoption preview PDF13. ; Note a: unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; Blanks shall not be filled with zero or guessed as residual limits. ; Note b: sulfur morphology/performance exceptions apply only to X3CrNiMoN27-5-2 and cannot be relaxed to .030 for all duplex steels. ; Note c: for X2CrNiMoN22-5-3 only, PRE>34 may be specified by agreement between both parties; the inequality is strict; PRE=Cr+3.3Mo+16N is the pitting resistance equivalent, which differs from carbon equivalents such as IIW. ; Asterisks in the original table indicate patented grades; no judgment is made on current patent validity or supply rights. ; A grade-listing standard does not independently establish delivery properties for a specific product, cold-heading suitability or the company’s ability to supply it; Adoptions of standards from other countries still require individual verification.

Verification notes

The official adoption relationship and original same-designation EN table have been checked; The complete French main text has not been checked page by page

X2CrNiMoCuN25-6-3 · EN 10088-1-2005

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10088-1-2005
Table / clause
Table 5, note a/b/c and asterisks, covering all 9 duplex corrosion-resistant steel grades
PDF page references
1、3、13

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
N0.2 ~ 0.3
Cr24.0 ~ 26.0
Cu1.0 ~ 2.5
Mo3.0 ~ 4.0
Ni6.0 ~ 8.0

Applicability and limitations

EN10088-1:2005 Table 5 duplex (austenitic-ferritic) corrosion-resistant stainless steels, heat analysis wt%; Official SIST adoption preview PDF13. ; Note a: unlisted elements must not be intentionally added without purchaser consent, except additions needed to finish the heat; Blanks shall not be filled with zero or guessed as residual limits. ; Note b: sulfur morphology/performance exceptions apply only to X3CrNiMoN27-5-2 and cannot be relaxed to .030 for all duplex steels. ; Note c: for X2CrNiMoN22-5-3 only, PRE>34 may be specified by agreement between both parties; the inequality is strict; PRE=Cr+3.3Mo+16N is the pitting resistance equivalent, which differs from carbon equivalents such as IIW. ; Asterisks in the original table indicate patented grades; no judgment is made on current patent validity or supply rights. ; A grade-listing standard does not independently establish delivery properties for a specific product, cold-heading suitability or the company’s ability to supply it; Adoptions of standards from other countries still require individual verification.

Verification notes

All 9 rows and footnotes in original Table 5 were visually checked

X2CrNiMoCuN25-6-3 · DIN EN 10088-3-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · EN 10028-7-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · EN 10088-2-2024

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · EN 10088-3-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · EN 10088-3-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · EN 10272-2016

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · NF EN 10028-7-2000

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo2.7 ~ 4
N0.15 ~ 0.3
Ni5.5 ~ 7.5
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · NF EN 10028-7-2008

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · NF EN 10088-2-2005

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · ISO 15510-2014

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · ISO 9328-7-2018

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo3 ~ 4
N0.2 ~ 0.3
Ni6 ~ 8
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

X2CrNiMoCuN25-6-3 · ISO TS 15510-2003

Original-source verification is incomplete; this is not a formal standard reference

Material category
Stainless steel
Subcategory
Duplex stainless steel
Material form
Reference record
Verification status
Reference data; original source not verified

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.03 (lower limit not stated)
Cr24 ~ 26
Cu1 ~ 2.5
Mn≤ 2 (lower limit not stated)
Mo2.5 ~ 4
N0.15 ~ 0.3
Ni5 ~ 7.5
P≤ 0.035 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Si≤ 0.7 (lower limit not stated)

Applicability and limitations

A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.

WhatsApp Technical enquiry →