X15CRNISI20-12
15 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for X15CRNISI20-12 →Material demand assessment
Looking for X15CRNISI20-12 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
X15CrNiSi20-12 · EN 10095-1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10095:1999
- Table / clause
- Table 2 and footnotes; complete historical original edition
- PDF page references
- 1、15、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 11.0 ~ 13.0 |
| N | ≤ 0.11 (lower limit not stated) |
Applicability and limitations
Original historical EN 10095:1999, Table 1—3 gives heat-analysis mass fractions wt%; This source is a scan of that original edition and must not be identified as DIN EN 10095:2018-12. ; Unlisted elements are not treated as zero and must not be intentionally added without purchaser consent, except additions needed to finish steelmaking. ; Specific supply form, heat treatment, properties and cold-heading suitability require separate verification against the product standard, contract and material certificate.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
EN 10095:1999 original Table 2 visually checked row by row; kept distinct from the 2018 German adopted edition.X15CrNiSi20-12 · DIN EN 10095-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10095:2018-12
- Table / clause
- Table 2, footnotes 1/*; 7.2
- PDF page references
- 1、2、3、9、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 11.0 ~ 13.0 |
| N | ≤ 0.11 (lower limit not stated) |
Applicability and limitations
DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply. 2018 national-foreword correction: Si1.50–2.50%; the earlier German 1.50–2.00 has been corrected.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
Official original DIN EN 10095:2018-12 composition and footnotes have been checked; Spacing within grade designations is normalized for correspondence; the EN year and DIN correction date are retained separately.X15CrNiSi20-12 · DIN EN 10095-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10095:2018-12
- Table / clause
- Table 2, footnotes 1/*; 7.2
- PDF page references
- 1、2、3、9、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 11.0 ~ 13.0 |
| N | ≤ 0.11 (lower limit not stated) |
Applicability and limitations
DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply. 2018 national-foreword correction: Si1.50–2.50%; the earlier German 1.50–2.00 has been corrected.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
Official original DIN EN 10095:2018-12 composition and footnotes have been checked; Spacing within grade designations is normalized for correspondence; the EN year and DIN correction date are retained separately.X15CrNiSi20-12 · EN 10095-1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10095:1999
- Table / clause
- Table 2 and footnotes; complete historical original edition
- PDF page references
- 1、15、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 11.0 ~ 13.0 |
| N | ≤ 0.11 (lower limit not stated) |
Applicability and limitations
Original historical EN 10095:1999, Table 1—3 gives heat-analysis mass fractions wt%; This source is a scan of that original edition and must not be identified as DIN EN 10095:2018-12. ; Unlisted elements are not treated as zero and must not be intentionally added without purchaser consent, except additions needed to finish steelmaking. ; Specific supply form, heat treatment, properties and cold-heading suitability require separate verification against the product standard, contract and material certificate.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
EN 10095:1999 original Table 2 visually checked row by row; kept distinct from the 2018 German adopted edition.X15CrNiSi20-12 · DIN EN 10095-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10095:2018-12
- Table / clause
- Table 2, footnotes 1/*; 7.2
- PDF page references
- 1、2、3、9、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 11.0 ~ 13.0 |
| N | ≤ 0.11 (lower limit not stated) |
Applicability and limitations
DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply. 2018 national-foreword correction: Si1.50–2.50%; the earlier German 1.50–2.00 has been corrected.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
All 26 chemical-composition rows and applicable footnotes in the official German text dated 2018-12 were checked; the 2018 corrigendum and product-analysis deviations are recorded separately.X15CrNiSi20-12 · EN 10095-1999
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- EN 10095:1999
- Table / clause
- Table 2 and footnotes; complete historical original edition
- PDF page references
- 1、15、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 19.0 ~ 21.0 |
| Ni | 11.0 ~ 13.0 |
| N | ≤ 0.11 (lower limit not stated) |
Applicability and limitations
Original historical EN 10095:1999, Table 1—3 gives heat-analysis mass fractions wt%; This source is a scan of that original edition and must not be identified as DIN EN 10095:2018-12. ; Unlisted elements are not treated as zero and must not be intentionally added without purchaser consent, except additions needed to finish steelmaking. ; Specific supply form, heat treatment, properties and cold-heading suitability require separate verification against the product standard, contract and material certificate.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat
Verification notes
EN 10095:1999 original Table 2 visually checked row by row; kept distinct from the 2018 German adopted edition.X15CrNiSi20-12 · DIN EN 10296-2-2006
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| N | ≤ 0.11 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · EN 10296-2-2005
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| N | ≤ 0.11 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · NF EN 10088-1-2005
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| N | ≤ 0.11 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · NF EN 10296-2-2005
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| N | ≤ 0.11 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · ISO 15510-2014
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| N | ≤ 0.1 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · ISO 4955-1994
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · ISO 4955-2005
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| N | ≤ 0.11 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · ISO 4955-2016
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Alloy steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| N | ≤ 0.1 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.
X15CrNiSi20-12 · SEW 470(1976)
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Verification status
- Reference data; original source not verified
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.2 (lower limit not stated) |
| Cr | 19 ~ 21 |
| Mn | ≤ 2 (lower limit not stated) |
| Ni | 11 ~ 13 |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.03 (lower limit not stated) |
| Si | 1.5 ~ 2.5 |
Applicability and limitations
A match in the materials database does not establish suitability for cold heading or guarantee finished-product strength. Confirmation must consider wire condition, deformation, heat treatment and tests on actual parts.