← BackMaterial grade directory

X15CRMO5-1

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X15CRMO5-1 →

Material demand assessment

Looking for X15CRMO5-1 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X15CrMo5-1 · EN 10269-2013

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10269-2013
Table / clause
Table1 high-temperature steels and note a/b
PDF page references
18、19

Carbon-equivalent reference

IIW / CEV:0.9400–1.6433Known-element contribution; incomplete value; missing V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2450–0.5767Known-element contribution; incomplete value; missing Cu, Ni, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2750–0.6250Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.18 (lower limit not stated)
Si≤ 0.4 (lower limit not stated)
Mn0.3 ~ 0.8
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr4.0 ~ 6.0
Mo0.45 ~ 0.65

Applicability and limitations

Table 1 and Note a/b in the official BS English adoption of EN10269:2013; heat analysis, wt%. ; The Al column is total aluminum; Elements not listed shall not be filled as zero and shall not be intentionally added without the consent of the purchaser (except those required to complete the smelting process). ; Note b: Sulfur levels by agreement are available only for marked grades; ordinary, machining and welding conditions are retained separately.. ; Titanium-stabilized grade X6CrNiTiB18-10 shall simultaneously satisfy Ti≥5C and Ti≤.80; a single-item upper limit shall not replace a linked lower limit. ; Product-analysis deviations, mechanical properties, delivery heat treatment and suitability for cold heading require separate verification; this record is not automatically included in the supply offering..

Verification notes

Official English Table 1 and applicable footnotes were visually checked

X15CrMo5-1 · NF EN 10269:1999

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Alloy steel
Subcategory
Alloy steel
Material form
Reference record
Original record status
Original-standard record
Standard edition
NF EN 10269:1999
Table / clause
EN 10269:1999 Table 1 and footnotes 1 and 2
PDF page references
2、22、23

Carbon-equivalent reference

IIW / CEV:0.9400–1.6433Known-element contribution; incomplete value; missing V, Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.2450–0.5767Known-element contribution; incomplete value; missing Cu, Ni, V, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.2750–0.6250Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C≤ 0.18 (lower limit not stated)
Si≤ 0.4 (lower limit not stated)
Mn0.3 ~ 0.8
P≤ 0.025 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr4.0 ~ 6.0
Mo0.45 ~ 0.65

Applicability and limitations

The cover of NF EN 10269:1999 explicitly adopts EN 10269:1999; Preserve the correspondence between the French adoption version and the European version; do not label as other countries or new editions. ; Table 1 gives heat-analysis mass percentages; Single values in P and S columns are upper limits; other single values are parsed according to the inequality signs in the original table; Unspecified elements shall not be filled as zero. ; Applies to billets, bars and wire rod of steels and nickel alloys for fasteners with specified high- or low-temperature properties.; Cold heading and actual supply must be verified in conjunction with delivery condition, dimensions, and process. ; Table 1 Footnote 1: Elements not listed in the table shall not be intentionally added without the buyer's consent (except additions needed to finish steelmaking); Elements that affect properties must be prevented from being introduced via scrap steel, etc.. ; This record only verifies the heat analysis composition in Table 1; product analysis tolerances in Table 2 shall not be automatically added to the heat limits.

Combined limits

Combined-element limits
    WhatsApp Technical enquiry →