X12NICRSI 35-16
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for X12NICRSI 35-16 →Material demand assessment
Looking for X12NICRSI 35-16 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
X12NiCrSi 35-16 · DIN EN 10095-2018
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Stainless steel
- Subcategory
- Austenitic stainless steel
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- DIN EN 10095:2018-12
- Table / clause
- Table 2, footnotes 1/*; 7.2
- PDF page references
- 1、2、3、9、16
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.15 (lower limit not stated) |
| Si | 1.0 ~ 2.0 |
| Mn | ≤ 2.0 (lower limit not stated) |
| P | ≤ 0.045 (lower limit not stated) |
| S | ≤ 0.015 (lower limit not stated) |
| Cr | 15.0 ~ 17.0 |
| Ni | 33.0 ~ 37.0 |
| N | ≤ 0.11 (lower limit not stated) |
Applicability and limitations
DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat