← BackMaterial grade directory

X10CRALSI13

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X10CRALSI13 →

Material demand assessment

Looking for X10CRALSI13 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X10CrAlSi13 · DIN EN 10095-2018

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
DIN EN 10095:2018-12
Table / clause
Table 1,footnote 1;7.2
PDF page references
1、2、3、9、15

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Si0.7 ~ 1.4
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr12.0 ~ 14.0
Al0.7 ~ 1.2

Applicability and limitations

DIN EN 10095:2018-12 is the German-language edition of EN 10095:1999 and includes the corrigenda listed in the national foreword; The national publication edition and adopted EN year are retained. Table 1–3 gives heat-analysis mass fractions wt%; 7.2.2 product-analysis tolerances are in Table 4/5 separately and must not be added to this heat-analysis range. Footnote 1: unlisted elements must not be intentionally added without purchaser consent, except for deoxidation; Unspecified content does not mean zero. Applicable to technical conditions for heat-resistant steels; this does not establish cold-heading suitability or product supply.

Verification notes

All 26 chemical-composition rows and applicable footnotes in the official German text dated 2018-12 were checked; the 2018 corrigendum and product-analysis deviations are recorded separately.

X10CrAlSi13 · EN 10095-1999

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Stainless steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
EN 10095:1999
Table / clause
Table 1 and footnotes; complete historical original edition
PDF page references
1、15

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.12 (lower limit not stated)
Si0.7 ~ 1.4
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr12.0 ~ 14.0
Al0.7 ~ 1.2

Applicability and limitations

Original historical EN 10095:1999, Table 1—3 gives heat-analysis mass fractions wt%; This source is a scan of that original edition and must not be identified as DIN EN 10095:2018-12. ; Unlisted elements are not treated as zero and must not be intentionally added without purchaser consent, except additions needed to finish steelmaking. ; Specific supply form, heat treatment, properties and cold-heading suitability require separate verification against the product standard, contract and material certificate.

Verification notes

EN 10095:1999 original Table 1 visually checked row by row; kept distinct from the 2018 German adopted edition.