← BackMaterial grade directory

X108CRMO17

2 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for X108CRMO17 →

Material demand assessment

Looking for X108CRMO17 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

X108CrMo17 · ISO 683-17-2014

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Bearing steel
Subcategory
Bearing steel
Material form
Reference record
Composition basis
Standard heat-analysis composition
Original record status
Original standard verified
Standard edition
ISO 683-17-2014
Table / clause
Table 3 and footnotes a–k
PDF page references
15、16
Unit
mass fraction (wt%)
Analysis type
Heat analysis; oxygen analysis is separately subject to the manufacturer’s choice

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default heat composition in the original table
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat composition in the original table; Agreed machinability: S≤0.030%
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr16.0 ~ 18.0
Mo0.4 ~ 0.8

Applicability and limitations

ISO 683-17:2014 Table 3 and footnotes checked against the original; Table 3 specifies heat analysis, mass fraction wt%; unspecified elements are not treated as zero. Product-analysis deviations are addressed separately in Table 4 and do not expand the default heat-analysis limits.

Composition conditions

Conditional requirement

Original condition-branch records

Default heat composition in the original table

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr16.0 ~ 18.0
Mo0.4 ~ 0.8

Default heat composition in the original table; Agreed machinability: S≤0.030%

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.0 ~ 18.0
Mo0.4 ~ 0.8

A condition branch must be selected

Yes

Verification notes

This batch was reconciled against the 2015 DIN German original images and 2014 ISO English original images; edition-specific sources were kept separate, and outdated grades, values and footnote scopes were corrected.

X108CrMo17 · DIN EN ISO 683-17-2015

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Bearing steel
Subcategory
Bearing steel
Material form
Reference record
Composition basis
Standard heat-analysis composition
Original record status
Original standard verified
Standard edition
DIN EN ISO 683-17:2015-02
Table / clause
Table 3 and footnotes a–k
PDF page references
19
Unit
mass fraction (wt%)
Analysis type
Heat analysis; oxygen analysis is separately subject to the manufacturer’s choice

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Default heat composition in the original table
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.
Default heat composition in the original table; Agreed machinability: S≤0.030%
Applicability of the three welding carbon-equivalent formulas has not been confirmed individually for each bearing-steel group. Only composition is shown; no carbon equivalent from standard ranges is automatically provided.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr16.0 ~ 18.0
Mo0.4 ~ 0.8

Applicability and limitations

DIN EN ISO 683-17:2015-02 Table 3 and footnotes checked against the original; the original Table 3 specifies heat analysis, mass fraction wt%; unspecified elements are not treated as zero. Product-analysis deviations are addressed separately in Table 4 and do not expand the default heat-analysis limits.

Composition conditions

Conditional requirement

Original condition-branch records

Default heat composition in the original table

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.015 (lower limit not stated)
Cr16.0 ~ 18.0
Mo0.4 ~ 0.8

Default heat composition in the original table; Agreed machinability: S≤0.030%

ElementComposition requirement
C0.95 ~ 1.2
Si≤ 1.0 (lower limit not stated)
Mn≤ 1.0 (lower limit not stated)
P≤ 0.04 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Cr16.0 ~ 18.0
Mo0.4 ~ 0.8

A condition branch must be selected

Yes

Verification notes

This batch was reconciled against the 2015 DIN German original images and 2014 ISO English original images; edition-specific sources were kept separate, and outdated grades, values and footnote scopes were corrected.
WhatsApp Technical enquiry →