← BackMaterial grade directory

W9MO3CR4V

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for W9MO3CR4V →

Material demand assessment

Looking for W9MO3CR4V material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

W9Mo3Cr4V · GB/T 9943-2025

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Subcategory
High-speed tool steel
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 9943-2025
Table / clause
Table 1 · Notes a/b
PDF page references
7、8

Carbon-equivalent reference

Estimates are presented separately for each applicable composition condition. Match the actual ordering conditions; ranges must not be combined.

Table 1 heat analysis, excluding electroslag-remelted steel
IIW / CEV:2.3633–2.8167Known-element contribution; incomplete value; missing Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):1.2867–1.5133Known-element contribution; incomplete value; missing Cu, Ni, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:1.2500–1.4600Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.
Table 1, note a: no Si minimum is specified for electroslag-remelted steel
IIW / CEV:2.3633–2.8167Known-element contribution; incomplete value; missing Ni, Cu CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):1.2800–1.5133Known-element contribution; incomplete value; missing Cu, Ni, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:1.2500–1.4600Known-element contribution; incomplete value; missing Cu, Ni CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition record (conditional branches apply; this is not an unconditional requirement)

ElementComposition requirement
C0.77 ~ 0.87
Si0.2 ~ 0.4
Mn0.2 ~ 0.4
Cr3.8 ~ 4.4
Mo2.7 ~ 3.3
V1.3 ~ 1.7
W8.5 ~ 9.5
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)

Applicability and limitations

GB/T9943-2025, Table 1, heat analysis, mass percent. ; Note a: No lower limit for Si in ESR steel; ranges of other elements shall not be changed because of this. ; Note b: Special S requirements may be specified in the contract to improve machining performance; since specific values are not provided, the general special S range shall not be filled in arbitrarily. ; Clause 7.1.2: Product-analysis tolerances are specified in Table 2; the heat-analysis limits have not been automatically expanded.. ; High-speed tool steel standards are not proof of suitability for cold-heading wire; Do not automatically add this to the range of cold-heading products available for supply..

Original condition-branch records

Table 1 heat analysis, excluding electroslag-remelted steel

ElementComposition requirement
C0.77 ~ 0.87
Si0.2 ~ 0.4
Mn0.2 ~ 0.4
Cr3.8 ~ 4.4
Mo2.7 ~ 3.3
V1.3 ~ 1.7
W8.5 ~ 9.5
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)

Table 1, note a: no Si minimum is specified for electroslag-remelted steel

ElementComposition requirement
C0.77 ~ 0.87
Si≤ 0.4 (lower limit not stated)
Mn0.2 ~ 0.4
Cr3.8 ~ 4.4
Mo2.7 ~ 3.3
V1.3 ~ 1.7
W8.5 ~ 9.5
P≤ 0.03 (lower limit not stated)
S≤ 0.02 (lower limit not stated)