1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for VDM NICKEL 201 →Material demand assessment
Looking for VDM NICKEL 201 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
VDM Nickel 201 · No corresponding standard is provided
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Nickel and nickel alloys
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Composition basis
- Manufacturer-published composition range
- Verification status
- Reference data; original source not verified
- Document title
- Material Data Sheet No.1101 Revision02 March2022
- Table / clause
- Table2b Chemical composition (%)
- PDF page references
- 3
- Manufacturer
- VDM Metals
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| C | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.005 (lower limit not stated) |
| Ni | ≥ 99.2 (upper limit not stated) |
| Mn | ≤ 0.35 (lower limit not stated) |
| Si | ≤ 0.15 (lower limit not stated) |
| Ti | ≤ 0.1 (lower limit not stated) |
| Cu | ≤ 0.25 (lower limit not stated) |
| Fe | ≤ 0.4 (lower limit not stated) |
| Mg | ≤ 0.15 (lower limit not stated) |
Applicability and limitations
Manufacturer data Table 2b is for Nickel201 composition; the C upper limit of Nickel200 is not applied. Ni is only specified with a lower limit of 99.2%; no separate upper limit is provided. May contain other unlisted elements.