VDM ALLOY 602 CA
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for VDM ALLOY 602 CA →Material demand assessment
Looking for VDM ALLOY 602 CA material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
VDM Alloy 602 CA · No corresponding standard is provided
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Nickel and nickel alloys
- Material form
- Reference record
- Composition basis
- Manufacturer-published composition range
- Verification status
- Reference data; original source not verified
- Document title
- Material Data Sheet No.4137 Revision04 March2022
- Table / clause
- Table2 Chemical composition according to DIN EN10302
- PDF page references
- 3
- Manufacturer
- VDM Metals
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Ni | Balance |
| Cr | 24 ~ 26 |
| Fe | 8 ~ 11 |
| C | 0.15 ~ 0.25 |
| Mn | ≤ 0.5 (lower limit not stated) |
| Si | ≤ 0.5 (lower limit not stated) |
| Cu | ≤ 0.1 (lower limit not stated) |
| Al | 1.8 ~ 2.4 |
| Ti | 0.1 ~ 0.2 |
| Y | 0.05 ~ 0.12 |
| Zr | 0.01 ~ 0.1 |
| P | ≤ 0.02 (lower limit not stated) |
| S | ≤ 0.01 (lower limit not stated) |
Applicability and limitations
Manufacturer Table 2 lists composition according to DIN EN10302, Mn≤0.50%; Footnote specifies Mn≤0.15% for UNS scope; other specifications may differ. The current table only displays the DIN EN10302 scope and does not automatically apply UNS or ASTM standards; the original text of specific versions shall be verified separately. Ni is the balance.