← BackMaterial grade directory

UHS1970

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for UHS1970 →

Material demand assessment

Looking for UHS1970 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

UHS1970 · Kobe Steel manufacturer specification (section 6-3)

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Spring steels
Subcategory
Spring steels
Material form
Wire rod
Original record status
Manufacturer source verified
Document edition
Publication edition not stated in the document
Document title
Wire rod and bar specification tables
Table / clause
6-3
PDF page references
25
Unit
Mass fraction (wt%)
Manufacturer
Kobe Steel

Carbon-equivalent reference

Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.

IIW / CEV:0.6733–0.8483Known-element contribution; incomplete value; missing Mo CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15; an engineering estimate of welding cold-cracking susceptibility for carbon and low-alloy steels.
Pcm(Ito–Bessyo):0.5425–0.6375Known-element contribution; incomplete value; missing Mo, B Pcm = C + Si/30 + (Mn + Cu + Cr)/20 + Ni/60 + Mo/15 + V/10 + 5B; mainly used for low-carbon low-alloy steels, particularly modern low-carbon pipeline steels; more relevant when C is approximately no higher than 0.11%.
CET:0.4800–0.5775Known-element contribution; incomplete value; missing Mo CET = C + (Mn + Mo)/10 + (Cr + Cu)/20 + Ni/40; used in welding preheat assessment for ferritic steels, subject to the applicability conditions of EN 1011-2.

Composition

ElementComposition requirement
C0.4 ~ 0.44
Si1.85 ~ 2.05
Mn0.1 ~ 0.45
P≤ 0.02 (lower limit not stated)
S≤ 0.02 (lower limit not stated)
Cu0.2 ~ 0.4
Ni0.5 ~ 0.7
Cr0.95 ~ 1.1
V0.1 ~ 0.2
Ti0.05 ~ 0.09

Applicability and limitations

Original composition in the Kobe Steel wire-rod catalogue, section 6-3 (PDF page 25), mass fractions wt%; This is not the original JIS/SAE standard. The manufacturer catalogue does not state a publication year; delivery condition, procurement availability and specific application require separate confirmation; This does not establish a supply commitment from Creation Group.

Composition conditions

Verification notes

Steel designations, elements and bounds in the original manufacturer catalogue table were visually checked cell by cell; Dashes are not filled with zero.