UHS1900M
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for UHS1900M →Material demand assessment
Looking for UHS1900M material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
UHS1900M · Kobe Steel manufacturer specification (section 6-3)
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Spring steels
- Subcategory
- Spring steels
- Material form
- Wire rod
- Original record status
- Manufacturer source verified
- Document edition
- Publication edition not stated in the document
- Document title
- Wire rod and bar specification tables
- Table / clause
- 6-3
- PDF page references
- 25
- Unit
- Mass fraction (wt%)
- Manufacturer
- Kobe Steel
Carbon-equivalent reference
Estimate from manufacturer-published ranges, not a standard guarantee or measured heat result; formula applicability requires review against the application and process.
Composition
| Element | Composition requirement |
|---|---|
| C | 0.46 ~ 0.49 |
| Si | 1.9 ~ 2.1 |
| Mn | 0.6 ~ 0.9 |
| P | ≤ 0.025 (lower limit not stated) |
| S | ≤ 0.025 (lower limit not stated) |
| Cu | 0.15 ~ 0.25 |
| Ni | 0.2 ~ 0.4 |
| Cr | 0.15 ~ 0.25 |
| V | 0.125 ~ 0.175 |
| Ti | 0.055 ~ 0.09 |
Applicability and limitations
Original composition in the Kobe Steel wire-rod catalogue, section 6-3 (PDF page 25), mass fractions wt%; This is not the original JIS/SAE standard. The manufacturer catalogue does not state a publication year; delivery condition, procurement availability and specific application require separate confirmation; This does not establish a supply commitment from Creation Group.
Composition conditions
- Original-table mass percentage, Section 6-3; Dashes and unlisted elements are not entered as zero.
- The manufacturer catalogue does not identify the publication edition; Catalogue information does not establish current supply dimensions.