← BackMaterial grade directory

TZR0.15

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for TZR0.15 →

Material demand assessment

Looking for TZR0.15 material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

TZr0.15 · GB/T 5231-2012

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material category
Copper and copper alloys
Material form
Reference record
Original record status
Original standard verified
Standard edition
GB/T 5231-2012
Table / clause
Table 1, row 28, designation C15000
PDF page references
5
Unit
Mass fraction (wt%)

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
Zr0.1 ~ 0.2

Applicability and limitations

Mass fraction wt%; GB/T 5231-2012, Table 1, row 28, designation C15000; original scan PDF page 5 (printed page 3). A dash indicates that the value is unspecified and shall not be treated as zero; The combined lower limit shall not be split into independent lower limits for each element. Standard Clause 2.2: Impurities listed as a single value in the table are maximum limits; Limits for elements not listed cannot be supplemented as zero by referring to other versions. Table 1 Note a: As, Bi, and Sb may not be analyzed, but the supplier must guarantee that they do not exceed the upper limits listed in the table. This standard only specifies the grades and chemical compositions of wrought copper and copper alloys; actual supply of cold heading wire shall not be inferred therefrom. Table 1 Note l: For this grade, Cu+Ag+Zr is not less than 99.9%. Table 1 Note l: For this grade, the sum of Cu+Ag+Zr is not less than 99.9%; The lower limit for Cu+Ag listed in the table remains 99.80%.

Combined limits

Combined-element limits
  • Element coefficient
    Cu
    1
    Ag
    1
    Lower limit
    99.8
    Requirement
    Minimum total Cu + Ag
  • Element coefficient
    Cu
    1
    Ag
    1
    Zr
    1
    Lower limit
    99.9
    Requirement
    Table 1, note l: minimum combined Cu+Ag+Zr
Elements requiring measured values from the same heat
  • Ag
  • Cu
  • Zr

Verification notes

Each cell of Table 1 in the scanned original standard was checked manually; applicable footnotes are recorded separately.