TUAL0.12
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for TUAL0.12 →Material demand assessment
Looking for TUAL0.12 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
TUAl0.12 · GB/T 5231-2012
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Copper and copper alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5231-2012
- Table / clause
- Table 1, row 31, designation T15700
- PDF page references
- 5
- Unit
- Mass fraction (wt%)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| P | ≤ 0.002 (lower limit not stated) |
| Al2O3 | 0.16 ~ 0.26 |
| Bi | ≤ 0.001 (lower limit not stated) |
| Sb | ≤ 0.002 (lower limit not stated) |
| As | ≤ 0.002 (lower limit not stated) |
| Fe | ≤ 0.004 (lower limit not stated) |
| Ni | ≤ 0.002 (lower limit not stated) |
| Pb | ≤ 0.003 (lower limit not stated) |
| Sn | ≤ 0.002 (lower limit not stated) |
| S | ≤ 0.004 (lower limit not stated) |
| Zn | ≤ 0.003 (lower limit not stated) |
Applicability and limitations
Mass fraction wt%; GB/T 5231-2012, Table 1, row 31, designation T15700; original scan PDF page 5 (printed page 3). A dash indicates that the value is unspecified and shall not be treated as zero; The combined lower limit shall not be split into independent lower limits for each element. Standard Clause 2.2: Impurities listed as a single value in the table are maximum limits; Limits for elements not listed cannot be supplemented as zero by referring to other versions. Table 1 Note a: As, Bi, and Sb may not be analyzed, but the supplier must guarantee that they do not exceed the upper limits listed in the table. This standard only specifies the grades and chemical compositions of wrought copper and copper alloys; actual supply of cold heading wire shall not be inferred therefrom. Cu is the balance; Al2O3 refers to the alumina content and must not be mistaken for the element Al range.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat