TRIBALOY T-800
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for TRIBALOY T-800 →Material demand assessment
Looking for TRIBALOY T-800 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
Tribaloy T-800 · No corresponding standard is provided
Original-source verification is incomplete; this is not a formal standard reference
- Material category
- Stainless steel
- Subcategory
- Special alloy steel
- Material form
- Reference record
- Composition basis
- Manufacturer typical composition range
- Verification status
- Reference data; original source not verified
- Document title
- Tribaloy official web data; accessed2026-10-13
- Table / clause
- Tribaloy T-800 — Nominal Composition
- PDF page references
- Manufacturer
- Kennametal Stellite
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Co | Cobalt base (no numerical value stated) |
| Cr | Typical/nominal value 17.5 (not a guaranteed range) |
| Mo | Typical/nominal value 28.5 (not a guaranteed range) |
| Si | Typical/nominal value 3.4 (not a guaranteed range) |
| C | <0.08 (lower limit not stated) |
| Ni | Listed as another element; no numerical value stated |
| Fe | Listed as another element; no numerical value stated |
Applicability and limitations
The manufacturer's official website only lists nominal compositions: Cr 17.5%, Mo 28.5%, Si 3.4%; these single points are not permissible upper and lower limits and shall not be used for range reverse-lookup or standard guarantees.. C<0.08% is a strict upper limit.; Co is the base; Ni/Fe are listed as other elements but have no values.. N/O/P/S and Cr/Mo/Si ranges in the original reference library cannot be confirmed based on this table; original values are retained in the repair evidence. The manufacturer page lists both UNS/AMS as NotListed; do not invent identifiers..