TP309CB

1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.

Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.

Open condition selection, comparison and carbon-equivalent tools for TP309CB →

Material demand assessment

Looking for TP309CB material?

Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.

Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.

Explore products and processing capabilities

TP309Cb · ASME SA-814/SA-814M-2023

Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results

Material form
Reference record
Original record status
Original standard verified
Standard edition
ASME SA-814/SA-814M-2023
Table / clause
Table 2, notes A–H; clauses 5.1/5.2; identity statement on PDF page 1
PDF page references
1、4、5

Source document

Carbon-equivalent reference

IIW / CEV: not directly applicable to this material category
Pcm (Ito–Bessyo): not directly applicable to this material category
CET: not directly applicable to this material category

Composition

ElementComposition requirement
C≤ 0.08 (lower limit not stated)
Mn≤ 2.0 (lower limit not stated)
P≤ 0.045 (lower limit not stated)
S≤ 0.03 (lower limit not stated)
Si≤ 1.0 (lower limit not stated)
Ni12.0 ~ 16.0
Cr22.0 ~ 24.0

Applicability and limitations

Composition alloy: S30940. Table 2, mass fraction wt%; values are maxima except where explicit ranges are given. Ellipses are not replaced with zero. The source actually read is ASME BPVC.II.A-2023 SA814; the cover explicitly states that it is identical to ASTM A814/A814M-15(2019). The analytical method for N is subject to agreement between purchaser and supplier. Product-analysis tolerances under A480/A480M require separate verification and are not incorporated into this table. This standard covers cold-worked welded stainless steel pipe and does not automatically approve a cold-heading product.

Combined limits

Elements requiring measured values from the same heat
  • Nb
  • Ta
Combined-element limits
  • Element coefficient
    Nb
    1
    Ta
    1
    C
    -10
    Lower limit
    0
    Requirement
    Nb+Ta≥10C
  • Element coefficient
    Nb
    1
    Ta
    1
    Upper limit
    1.1
    Requirement
    Nb+Ta≤1.10%

Verification notes

Checked against the standard chemical-composition table and footnotes.
WhatsApp Technical enquiry →