TCR1-0.18
1 source records. Standards, editions and conditions are presented separately; matching grade names do not establish interchangeability.
Refer to each source for mass fractions and analysis type. Missing values are not treated as 0. Manufacturer typical values, standard guarantees and measured heat results must remain separate. Use the material selector for calculations and condition selection.
Open condition selection, comparison and carbon-equivalent tools for TCR1-0.18 →Material demand assessment
Looking for TCR1-0.18 material?
Not listed in our catalog? You are welcome to submit your requirements. We assess whether our equipment, production lines and process capabilities suit your grade, product form, dimensions, processing and delivery requirements, then discuss possible processing, trials or supply arrangements.
Feasibility and supply terms are confirmed after technical review. The standard information on this page is not a supply or performance commitment.
Keep your entries and try again later, or contact website@chqwire.net. If you have already received confirmation, do not submit again.
TCr1-0.18 · GB/T 5231-2012
Chemical composition source verified; this does not verify every standard clause, actual supply or measured heat results
- Material category
- Copper and copper alloys
- Material form
- Reference record
- Original record status
- Original standard verified
- Standard edition
- GB/T 5231-2012
- Table / clause
- Table 2, row 18, designation T18160
- PDF page references
- 6
- Unit
- Mass fraction (wt%)
Carbon-equivalent reference
Composition
| Element | Composition requirement |
|---|---|
| Zr | 0.05 ~ 0.3 |
| Cr | 0.5 ~ 1.5 |
| Si | ≤ 0.1 (lower limit not stated) |
| Fe | ≤ 0.1 (lower limit not stated) |
| Al | ≤ 0.05 (lower limit not stated) |
| Pb | ≤ 0.05 (lower limit not stated) |
| Mg | ≤ 0.05 (lower limit not stated) |
| P | ≤ 0.1 (lower limit not stated) |
| B | ≤ 0.02 (lower limit not stated) |
| Sb | ≤ 0.01 (lower limit not stated) |
| Bi | ≤ 0.01 (lower limit not stated) |
Applicability and limitations
Mass fraction wt%; GB/T 5231-2012, Table 2, row 18, designation T18160; original scan PDF page 6 (printed page 5). Where Cu is marked as the balance, no numerical range is invented; A dash means unspecified and must not be entered as zero. Clause 2.2: single tabulated impurity values are maxima; Manufacturer supply and the chemical composition in this standard require separate confirmation. Table 2, note a: high-copper alloys have copper content between 96.0% and 99.3%; This standard does not establish a guarantee of cold-heading wire supply. Tabulated total impurities ≤0.3%; this is not the maximum for each unlisted element. Table 2, note d: total impurities 0.3% are the sum of measured contents of the listed impurity elements, not the sum of their maxima.
Combined limits
- Combined-element limits
- Elements requiring measured values from the same heat